Research on High-speed Milling Transition Criteria and Chip Edge Formation Mechanism of DD5 Ni-based Single Crystal Superalloys

  • LI Qiang ,
  • GUO Chenguang ,
  • ZHAO Lijuan ,
  • LENG Yuefeng ,
  • YUE Haitao
Expand
  • School of Mechanical Engineering, Liaoning Technical University, Fuxin,Liaoning,123000

Received date: 2019-05-13

  Online published: 2020-10-21

Abstract

In order to improve the difficult-to-machine property of DD5 Ni-based single crystal superalloys, a high-speed milling transition criteria and chip edge formation mechanism were proposed with the variable of cutting speed based on adiabatic shear theory and using the method of single factor experiments and FEM simulation. According to the measurement results of the chip sawtooth level and intervals, the chip free surface transforms from lamellar structure to serrated structure when cutting speed reaches 37.7 m/min, which shows the milling has entered into high-speed zone. The stress concentrated on the grooves intersected between the chip side and adiabatic shear band induces the longitudinal crack formation and expansion, which causes the transverse and longitudinal stress distribution variations. Then, the transverse cracks were generated. The longitudinal and transverse crack formation was the main reason of the chip edge generation. With the increasing of milling speed, the chip edge morphology transformed from flat and smooth trapezoid to narrow and defective triangle. Compared with the traditional machining, high-speed cutting is beneficial to the reduction of cutting force, chip edge height and intervals, and restrain the lateral crack expansion at the same time.

Cite this article

LI Qiang , GUO Chenguang , ZHAO Lijuan , LENG Yuefeng , YUE Haitao .

Research on High-speed Milling Transition Criteria and Chip Edge Formation Mechanism of DD5 Ni-based Single Crystal Superalloys
[J]. China Mechanical Engineering, 2020 , 31(19) : 2388 -2393 . DOI: 10.3969/j.issn.1004-132X.2020.19.016

References

[1]IMRAN M, MATIVENGA P T, GHOLINIA A, et al. Comparison of Tool Wear Mechanisms and Surface Integrity for Dry and Wet Micro-drilling of Nickel-base Superalloys[J]. International Journal of Machine Tools and Manufacture, 2014, 76(1):49-60.
[2]ZHU D, ZHANG X M, DING H. Tool Wear Characteristics in Machining of Nickel-based Superalloys[J]. International Journal of Machine Tools and Manufacture, 2013, 64:60-77.
[3]THAKUR A, GANGOPADHYAY S. State-of-the-art in Surface Integrity in Machining of Nickel-based Super Alloys[J]. International Journal of Machine Tools and Manufacture, 2015, 100:25-54.
[4]刘丽娟,吕明,武文革,等.高速铣削钛合金Ti-6Al-4V切屑形态试验研究[J].机械工程学报,2015,51(3):196-205.
LIU Lijuan, LYU Ming,WU Wenge, et al. Experimental Study on the Chip Morpholgy in High Speed Milling Ti-6Al-4V Alloy[J]. Journal of Mechanical Engineering, 2015,51(3):196-205.
[5]孙涛,梁晋,李登万,等.高温合金高速精铣表面完整性建模及切削参数优化研究[J].中国机械工程,2017,28(16):1906-1913.
SUN Tao,LIANG Jin, LI Dengwan, et al. Study on Surface Integrity Modelling and Cutting Parameter Optimization of Superalloy in High-speed Finish Milling[J]. China Mechanical Engineering, 2017,28(16):1906-1913.
[6]CUI X, JIAO F, ZHAO B, et al. A Review of High-speed Intermittent Cutting of Hardened Steel[J]. International Journal of Advanced Manufacturing Technology, 2017, 93(4):1-10.
[7]MOLINARI A, MUSQUAR C, SUTTER G. Adiabatic Shear Banding in High Speed Machining of Ti-6Al-4V:Experiments and Modeling[J]. International Journal of Plasticity, 2002, 18(4):443-459.
[8]VYAS A, SHAW M C. Mechanics of Saw-tooth Chip Formation in Metal Cutting[J]. Journal of Manufacturing Science and Engineering, 1999, 121:163-172.
[9]SCHULZ H, ABELE E, SAHM A. Material Aspects of Chip Formation in HSC Machining[J]. CIRP Annals—Manufacturing Technology, 2001, 50(1):45-48.
[10]EKINOVIC'
 S, BEGOVIC' E. An Approach to Determine Transition Area from Conventional to High-speed Machining by Means of Chip Shape Analysis[J]. Archives of Materials Science, 2007, 28:35-39.
[11]吴明阳,于永新,程耀楠,等.高压冷却下锯齿形切屑几何表征试验[J].中国机械工程, 2019, 30(1):38-45.
WU Mingyang, YU Yongxin, CHENG Yaonan, et al. Geometrical Characterization Test of Serrated Chips under High-pressure Cooling[J]. China Mechanical Engineering, 2019, 30(1):38-45.
[12]LI Q, GONG Y D, SUN Y, et al. Milling Performance Optimization of DD5 Ni-based Single-crystal Superalloy[J]. The International Journal of Advanced Manufacturing Technology,2018,94:2875-2894.
[13]杜劲. 粉末高温合金FGH95高速切削加工表面完整性研究[D]. 济南:山东大学, 2012.
DU Jin. Surfece Integrity for High Speed Machining of Powder Metallurgy Superalloy FGH95[D]. Jinan:Shandong University, 2012.
[14]周俊. 镍基高温合金GH4169高速切削相关技术与机理的研究[D]. 哈尔滨:哈尔滨工业大学, 2012.
ZHOU Jun. Research on Correlation Technique and Mechanism of High-speed Cutting Ni-based Superalloy GH4169[D]. Harbin:Harbin Institute of Technology, 2012.
Outlines

/

〈 〉