The object herein was to investigate the effects of different grinding marks directions on the rail fatigue crack propagations under water medium conditions using a MMS-2A wheel/rail friction wear testing apparatus. And the different grinding marks angles to the running direction were manufactured on rail specimens by brown corundum sand. The results indicate that the surface roughness of rail specimen with the grinding marks angle of 0°~45° to the running direction is higher than that with the grinding marks angle of 7° and 90° under the water medium conditions. The grinding marks with the angle of 0°~45° to the running direction may accelerate the fatigue crack propagations compared with the smooth area on rail specimen without prefabricated grinding marks. And the crack propagation is particularly serious on the rail specimen surface with the angle of 20° grinding marks which has a lot of branch cracks. The growth of the fatigue cracks slows down for the rail specimen with the grinding marks angle of 70°, 90°, and there are only surface cracks on the rail specimen with the angle of 90° grinding marks. With the angle of grinding marks increases from 0° to 90°, the crack propagation depth of rail specimen increases firstly and then decreases, and the crack propagation angle tends to decrease gradually.
[1] 刘启跃, 王文健, 周仲荣.高速与重载铁路钢轨损伤及预防技术差异研究[J].润滑与密封,2007,32(11):11-14. LIU Qiyue, WANG Wenjian, ZHOU Zhongrong. An Investigation on Difference of Rail Damage and Preventive Technique of High-speed and Heavy-haul Railway[J]. Lubrication Engineering, 2007, 32(11):11-14.
[2] 刘启跃, 张波, 周仲荣. 铁路钢轨损伤机理研究[J]. 中国机械工程,2002,13(18):1596-1599. LIU Qiyue, ZHANG Bo, ZHOU Zhongrong. The Railway Rail Damage Mechanism[J]. China Mechanical Engineering, 2002, 13(18):1596-1599.
[3] 周仲荣. 关于微动磨损与微动疲劳的研究[J]. 中国机械工程,2002,11(10):1146-1150. ZHOU Zhongrong. The Study of Fretting Wear and Fretting Fatigue[J]. China Mechanical Engineering, 2002, 11(10):1146-1150.
[4] 王文健, 陈明韬, 郭俊, 等.高速铁路钢轨打磨技术及其应用[J].西南交通大学学报, 2007, 42(5):574-577. WANG Wenjian, CHEN Mingtao, GUO Jun, et al. Rail Grinding Technique and Its Application in High-speed Railway[J]. Journal of Southwest Jiaotong University, 2007, 42(5):574-577.
[5] 金学松, 杜星, 郭俊, 等.钢轨打磨技术研究进展[J].西南交通大学学报, 2010, 45(1):1-11. JIN Xuesong, DU Xing, GUO Jun, et al. State of Arts of Research on Rail Grinding[J]. Journal of Southwest Jiaotong University, 2010, 45(1):1-11.
[6] WANG W J, GUO J, LIU Q Y, et al. Study on Relationship between Oblique Fatigue Crack and Rail Wear in Curve Track and Prevention[J] Wear, 2009, 267:540-544.
[7] 顾凯凯, 王文健, 郭俊, 等.钢轨-石相互作用的摩擦学模拟试验研究[J].摩擦学学报,2015,35(2):154-159. GU Kaikai, WANG Wenjian, GUO Jun, et al. Tribological Simulation Experiment of Interactions between Rail and Grinding Stone[J]. Tribology, 2015, 35(2):154-159.
[8] 江晓禹, 金学松.轮轨间的液态介质和表面微观粗糙度对接触表面疲劳损伤的影响[J].机械工程学报,2004,40(8):18-23. JIANG Xiaoyu,JIN Xuesong. Influence of Liquid and Micro-roughness between Wheel and Rail on the Fatigue Damage of Contact Surface[J]. Chinese Journal of Mechanical Engineering, 2004, 40(8):18-23.
[9] 刘腾飞, 王文健, 郭火明, 等.不同介质对轮轨增黏与磨损特性影响[J].摩擦学学报,2014,34(2):153-159. LIU Tengfei, WANG Wenjian, GUO Huoming, et al. Effect of Medium on Improving Adhesion and Wear Characteristics of Wheel/Rail[J]. Tribology, 2014, 34(2):153-159.
[10] CHEN H, ISHIDA M. Influence of Rail Surface Roughness Formed by Rail Grinding on Rolling Contact Fatigue[J]. Quarterly Report of RTRI, 2006, 47(4):216-221.
[11] GAO N, DWYER-JOYCE R S. The Effects of Surface Defects on the Fatigue of Water-and Oil-lubricated Contacts[J]. Proc. Instn. Mech. Engrs., 2000, 214(J):611-626.
[12] GAO N, DWYER-Joyce R S, GRIEVE D G. Disc Machine Testing to Assess the Life of Surface-damaged Railway Track[J]. Proc. Instn. Mech. Engrs., 2001, 215(F):261-275.
[13] KHALLADI A, ELLEUCH K. Effect of Surface Topography with Different Groove Angles on Tribological Behavior of the Wheel/Rail Contact Using Alternative Machine[J]. Friction, 2016, 4(3):238-248.
[14] SVAHN F, KASSMAN-RUDOLPHI A, WALLEN E. The Influence of Surface Roughness on Friction and Wear of Machine Element Coatings[J]. Wear, 2003, 254(11):1092-1098.
[15] 蔡宝春, 蒋华臻, 王文中, 等.轮轨试样表面粗糙度取向对油润滑下摩擦系数的影响[J].力学学报, 2016,48(5):1114-1125 CAI Baochun, JIANG Huazhen, WANG Wenzhong, et al. Influence of Surface Roughness Orientations on Friction Coefficient of Wheel/rail Specimen in Oil Lubrication[J]. Chinese Journal of Theoretical and Applied Mechanics, 2016, 48(5):1114-1125.
[16] 方新燕. 三维表面形貌的表征及润滑特性的研究[D]. 合肥:合肥工业大学, 2006. FANG Xinyan. Characterization and Lubrication Analysis of Three-dimensional Surface Topography[D]. Hefei:Hefei University of Technology, 2006.
[17] TYFOUR W R, BEYNON J H, KAPOOR A. Deterioration of Rolling Contact Fatigue Life of Pearlitic Rail Steel due to Dry-wet Tolling-sliding Line Contact[J]. Wear, 1996, 197(1/2):255-265.
[18] BOGDANSKI S, OLZAK M, STUPNICKI J. The Effects of Face Friction and Tractive Force on Propagation of 3D Squat Type of Rolling Contact Fatigue Crack[C]//Proceedings of the Second Mini Conference on Contact Mechanics and Wear of Rail/Wheel Systems Budapes. Sydney,1996:164-173.
[19] LUNDEN R. Cracks in Railway Wheels under Rolling Contact Load[C]//Tenth International Wheelset Congress:Sharing the Latest Wheelset Technology in Order to Reduce Costs and Improve Railway Productivity.Sydney,1992:163-167.
[20] WONG S L, BOLD P E, BROWN M W, et al. A Branch Criterion for Shallow Angled Rolling Contact Fatigue Cracks in Rails[J]. Wear, 1996, 191(1/2):45-53.
[21] 杨志强,崔金磊,杨沛然.表面粗糙度纹理对非牛顿热弹流润滑性能的影响[J].润滑与密封,2008,33(4):8-11. YANG Zhiqiang, CUI Jinlei, YANG Peiran. Influence of Surface Roughness on the Lubricating Behavior of Elliptic EHL Contacts under Thermal Non-Newtonian Condition[J]. Lubrication Engineering, 2008, 33(4):8-11.
[22] 刘红彬. 表面纹理对油膜润滑影响的研究[D].北京:中国农业大学,2007 LIU Hongbin. The Study of the Influence of Surface Texture on Oil Film Lubrication[D]. Beijing:China Agricultural University, 2007.
[23] PATIR N, CHENG H S. Application of Average Flow Model to Lubrication between Rough Sliding Surfaces[J]. Lubri. Technol. Trans. ASME, 1979, 101(2):220-229.
[24] 李军. 弹塑性状态下复合型疲劳裂纹扩展研究[D].北京:北京理工大学,2014. LI Jun. A Study on Elastic-plastic Mixed-mode Fatigue Crack Propagation[D]. Beijing:China Beijing Institute of Technology, 2014.