磨粒技术专栏

多孔钎焊砂轮的制备及SiC陶瓷磨削试验研究

展开
  • 1.湖南科技大学机电工程学院,湘潭,411201
    2.湖南科技大学难加工材料高效精密加工湖南省重点实验室,湘潭,411201
刘伟,男,1986年生,副教授、博士。研究方向为高效精密智能磨削技术。发表论文30余篇。E-mail:lw1986tiger@163.com。

收稿日期: 2021-10-13

  网络出版日期: 2022-08-17

基金资助

国家自然科学基金(51505144);湖南省自然科学基金(2020JJ5178,2020JJ4024);湖南省教育厅科学研究项目(20A202,18A182);湖南省电磁装备设计与制造重点实验室开放基金(DC201901);难加工材料高效精密加工湖南省重点实验室开放基金(E22002)

Preparation of Porous Brazed Grinding Wheels and Experimental Research of SiC Ceramic Grinding

Expand
  • 1.School of Mechanical Engineering,Hunan University of Science and Technology,Xiangtan,Hunan,411201
    2.Hunan Provincial Key Laboratory of High Efficiency and Precision Machining of Difficult-to-cut  Material,Hunan University of Science and Technology,Xiangtan,Hunan,411201

Received date: 2021-10-13

  Online published: 2022-08-17

摘要

基于模压成形和真空固相烧结工艺,选用Cu-10Sn结合剂、经氧化预处理的TiH2钎焊造孔剂、MBD8金刚石磨粒,制备出磨粒把持力大、孔隙分布均匀的多孔钎焊金刚石砂轮(PBDGW)。开展PBDGW与多层钎焊金刚石砂轮(MBDGW)的SiC陶瓷磨削对比试验,从磨削力、工件表面粗糙度和表面/亚表面形貌等方面分析砂轮的磨削性能。试验结果表明:与MBDGW相比,PBDGW磨削SiC陶瓷的切向力下降了8.4%~23.6%、法向力下降了10.2%~38.6%,磨削加工表面粗糙度平均降幅为10.4%;工件表面完整性较好,表面/亚表面的脆性断裂、微观裂纹等缺陷较少。

本文引用格式

刘伟, 毛国安, 严灿, 李博鑫, . 多孔钎焊砂轮的制备及SiC陶瓷磨削试验研究[J]. 中国机械工程, 2022 , 33(15) : 1787 -1793 . DOI: 10.3969/j.issn.1004-132X.2022.15.004

Abstract

Based on the molding and vacuum solid-phase sintering processes,a porous brazed diamond grinding wheel(PBDGW)with high bonding strength and uniform pore distribution was prepared by using Cu-10Sn binder,oxidation pretreated TiH2 brazed pore-forming agent and MBD8 diamond abrasive particles. The SiC ceramic grinding experiments of PBDGW and multilayer brazed diamond grinding wheel(MBDGW) were carried out for comparison,then the grinding performances of grinding wheel were analyzed from grinding force,workpiece surface roughness and surface/sub-surface morphology. The experimental results show that the tangential force in SiC ceramics grinding with PBDGW decreases by 8.4%~23.6%,the normal force decreases by 10.2%~38.6%,and the average reduction of surface roughness is  as 10.4%. The workpiece surface has better integrity,and the surface/sub-surface brittle fracture,microscopic crack and other defects are less. 

参考文献

[1]ISHIHARA M,BABA S,TAKAHASHI T,et al.Fundamental Thermomechanical Properties of SiC-based Structural Ceramics Subjected to High Energy Particle Irradiations[J].Fusion Engineering and Design,2000,51:117-121.
[2]JI R J,LIU Y H,ZHANG Y Z,et al.Optimizing Machining Parameters of Silicon Carbide Ceramics with ED Milling and Mechanical Grinding Combined Process[J].The International Journal of Advanced Manufacturing Technology,2010,51(1):195-204.
[3]CAO J G,WU Y B,LU D,et al.Material Removal Behavior in Ultrasonic-assisted Scratching of SiC Ceramics with a Single Diamond Tool[J].International Journal of Machine Tools and Manufacture,2014,79:49-61.
[4]KHALID F,KLOTZ U,ELSENER H R,et al.On the Interfacial Nanostructure of Brazed Diamond Grits[J].Scripta Materialia,2004,50(8):1139-1143.
[5]姚正军,徐鸿钧,肖冰,等.Ni-Cr合金Ar气保护炉中钎焊金刚石砂轮的研究[J].中国机械工程,2001,12(8):956-958.
YAO Zhengjun,XU Hongjun,XIAO Bing,et al.Research on Furnace Brazing of Diamond Grinding Wheel with Ni-Cr Alloy under Argon Atmosphere[J].China Mechanical Engineering,2001,12(8):956-958.
[6]MUKHOPADHYAY P,GHOSH A.High Vacuum Brazing of Synthetic Diamond Grits with Steel Using Micro/Nano Al2O3 Reinforced Ag-Cu-Ti Alloy[J].Journal of Materials Processing Technology,2019,266:198-207.
[7]DUAN D Z,HAN F,DING J J,et al.Microstructure and Performance of Brazed Diamonds with Multilayer Graphene-modified Cu-Sn-Ti Solder Alloys[J].Ceramics International,2021,47(16):22854-22863.
[8]LOGINOV P,SIDORENKO D,SHVYNDINA N,et al.Effect of Ti and TiH2 Doping on Mechanical and Adhesive Properties of Fe-Co-Ni Binder to Diamond in Cutting Tools[J].International Journal of Refractory Metals and Hard Materials,2019,79:69-78.
[9]WANG C Y,ZHOU Y M,ZHANG F L,et al.Interfacial Microstructure and Performance of Brazed Diamond Grits with Ni-Cr-P Alloy[J].Journal of Alloys and Compounds,2008,476(1):884-888.
[10]AGARWAL S,RAO P V.Experimental Investigation of Surface/Subsurface Damage Formation and Material Removal Mechanisms in SiC Grinding[J].International Journal of Machine Tools and Manufacture,2007,48(6):698-710.
[11]WU C J,LI B Z,LIU Y,et al.Surface Roughness Modeling for Grinding of Silicon Carbide Ceramics Considering Co-existence of Brittleness and Ductility[J].International Journal of Mechanical Sciences,2017,133:167-177.
[12]TANAKA T.New Development of Metal Bonded Diamond Wheel with Pore by the Growth of Bonding Bridge[J].Japan Society for Precision Engineering,1992,26(1):27-32.
[13]吕冰海,董晨晨,邓乾发,等.可溶填充剂对孔隙自生成超硬磨料磨具孔隙生成的影响[J].机械工程学报,2014,50(15):172-179.
LYU Binghai,DONG Chenchen,DENG Qianfa,et al.Influence of Soluble Filler on Pores Self-generation Superabrasive Tool[J].Journal of Mechanical Engineering,2014,50(15):172-179.
[14]MATSUMARU K,TAKATA A.Fabrication of Porous Metal Bonded Diamond Grinding Wheels for Flat-surface Nanomachining[J].MRS Bulletin,2001,26(7):544-546.
[15]陈珍珍,徐九华,丁文锋,等.多孔复合结合剂立方氮化硼砂轮磨损特性[J].机械工程学报,2014,50(17):201-207.
CHEN Zhenzhen,XU Jiuhua,DING Wenfeng,et al.Wear Behavior of Porous Composite-bonded CBN Abrasive Wheels[J].Journal of Mechanical Engineering,2014,50(17):201-207.
[16]杨薇,温学兵,肖红,等.多孔金属结合剂CBN砂轮的研制及其高效磨削加工钛合金研究[J].航空制造技术,2019,62(20):64-69.
YANG Wei,WEN Xuebing,XIAO Hong,et al.Study on Design and Performance of Porous Metal-Bonded CBN Abrasive Wheels During Grinding of Ti-6Al-4V[J].Aeronautical Manufacturing Technology,2019,62(20):64-69.
[17]伍俏平,罗舟,邓朝晖,等.两种合金化铜基钎料真空钎焊金刚石[J].材料热处理学报,2018,39(3):151-158.
WU Qiaoping,LUO Zhou,DENG Zhaohui,et al.Vacuum Brazing of Diamonds with Two Kinds of Alloying Copper-based Filler Metals[J].Journal of Materials and Heat Treatment,2018,39(3):151-158.
[18]VISCUSI A,AMMENDOLA P,ASTARITA A,et al.Aluminum Foam Made via a New Method Based on Cold Gas Dynamic Sprayed Powders Mixed through Sound Assisted Fluidization Technique[J].Journal of Materials Processing Technology,2016,231:265-276.
[19]方吉祥,赵康,谷臣清.化学法制备Al2O3包覆TiH2颗粒发泡剂[J].中国有色金属学报,2002,12(6):1205-1209.
FANG Jixiang,ZHAO Kang,GU Chenqing.Preparation of Al2O3-coated TiH2Foaming Reagent by Chemical Method[J].The Chinese Journal of Nonferrous Metals,2002,12(6):1205-1209.
[20]左孝青,潘晓亮,寥明顺,等.氧化处理对TiH2分解特性及组织结构的影响[J].材料科学与工艺,2008,16(2):211-215.
ZUO Xiaoqing,PAN Xiaoliang,LIAO Mingshun,et al. Effects of Heat Treatment on TiH2 Decomposition Behavior and Microstructure[J].Materials Science and Technology,2008,16(2):211-215.
[21]PADURETS L,DOBROKHOTOVA Z,SHILOV A.Transformations in Titanium Dihydride Phase[J].International Journal of Hydrogen Energy,1999,24(2):153-156.
[22]高洪吾,刘士魁,赵彦波,等.加热氧化处理对TiH2释氢行为的影响[J].中国有色金属学报,2005,15(3):363-367.
GAO Hongwu,LIU Shikui,ZHAO Yanbo,et al.Effect of Heat Oxidation Treatment on Gas Release Behavior of TiH2[J].The Chinese Journal of Nonferrous Metals,2005,15(3):363-367.
[23]魏莉,姚广春,张晓明,等.粉末冶金法制备多孔金属材料技术[J].材料导报,2004,18(7):15-18.
WEI Li,YAO Guangchun,ZHANG Xiaoming,et al.The Powder Metallurgic Technology of Preparing Foamed Metal Material[J].Materials Review,2004,18(7):15-18.
[24]左孝青,KEENEDY A R,毕业顺,等.小孔径泡沫铝的制备及孔结构细化机理[J].中国有色金属学报,2009,19(4):682-688.
ZUO Xiaoqing,KEENEDY A R,BI Yeshun,et al.Fabricating and Cell Structure Refining Mechanism of Aluminum Foam with Fine Cell Structure[J].The Chinese Journal of Nonferrous Metals,2009,19(4):682-688.
[25]曹建国,张勤俭.碳化硅陶瓷超声振动辅助磨削材料去除特性研究[J].机械工程学报,2019,55(13):205-211.
CAO Jianguo,ZHANG Qinjian.Material Removal Behavior in Ultrasonic Assisted Grinding of SiC Ceramics[J].Journal of Mechanical Engineering,2019,55(13):205-211.
文章导航

/

〈 〉