极端环境表面工程的科学问题

激光熔覆工艺参数对铁基双层涂层组织和残余应力的影响

展开
  • 1.中国矿业大学机电工程学院,徐州,221116
    2.军事科学院国防科技创新研究院,北京,100071
    3.徐州华恒机器人系统有限公司,徐州,221137
周嘉利,男,1996年生,博士研究生。研究方向为激光熔覆再制造。E-mail:zhoujl312@163.com。

收稿日期: 2021-08-30

  网络出版日期: 2022-07-22

基金资助

国家重点研发计划(2018YFC1902400); 国家自然科学基金(51676205); 江苏省科技计划(BE2019032); 江苏高校优势学科建设工程

Effects of Laser Cladding Process Parameters on Microstructure and Residual Stresses of Fe-based Double Layer Coatings

Expand
  • 1.School of Mechatronic Engineering,China University of Mining and Technology,Xuzhou,Jiangsu,221116
    2.National Innovation Institute of Defense Technology,Academy of Military Science PLA China,Beijing,100071
    3.Xuzhou Huaheng Robot System Co.,Ltd.,Xuzhou,Jiangsu,221137

Received date: 2021-08-30

  Online published: 2022-07-22

摘要

针对激光熔覆过程中剧烈的温度场变化伴随着应力、应变演化,进而导致零件具有高裂纹敏感性的问题,对不同激光扫描路径及工艺参数下残余应力演变规律进行研究。采用激光熔覆在Q345钢上制备了Fe基双层多道涂层,并以X射线衍射法结合电化学腐蚀剥层法测量沿涂层深度方向的残余应力分布,探究激光扫描路径、功率以及扫描速度对涂层显微组织和应力分布的影响。结果表明:涂层表面和内部为残余压应力,在涂层基体熔合线处残余应力发生突变,热影响区表现为残余拉应力;激光熔覆工艺对涂层残余应力的大小和分布规律有显著影响,当激光扫描路径为轮廓偏置式、激光功率为1.8 kW、扫描速度为0.02 m/s时,涂层具有最优的残余应力分布和成形质量;残余应力的产生主要与激光束对熔池的冲击作用以及熔覆层的非平衡凝固特性有关。

本文引用格式

周嘉利, 程延海, 陈永雄, 梁秀兵, 白成杰, 杜望 . 激光熔覆工艺参数对铁基双层涂层组织和残余应力的影响[J]. 中国机械工程, 2022 , 33(12) : 1418 -1426,1434 . DOI: 10.3969/j.issn.1004-132X.2022.12.002

Abstract

 Aiming at the problems that the components had high crack sensitivity due to the intense temperature field changes accompanied by stress and strain evolution in laser cladding processes. The evolution of residual stresses under different laser scanning paths and processing parameters was studied. Fe-based multilayer coatings were prepared by laser cladding on Q345 steels. The residual stress distribution along the coating depth was measured by X-ray diffraction method combined with electrochemical corrosion stripping method. The effects of laser scanning path, power and scanning speed on the microstructure and stress distribution of the coatings were investigated. The results show that the residual compressive stress occurs on the surface and inside of the coatings, the residual stresses changes at the coating-substrate fusion line, and the heat-affected zones are of the residual tensile stress. Laser cladding processes have significant influences on the size and distribution of residual stresses for coatings. When laser scanning path is contour bias, power is as 1.8 kW and scanning speed is as 0.02 m/s, the coatings have the best residual stress distribution and forming quality. The residual stress is mainly related to the impacts of laser beams on the molten pool and the non-equilibrium solidification characteristics of the cladding layers.

参考文献

[1]NING B, LIU H, CUI J B, et al. Failure Analysis of Center Cutter Mount in Shield Machine under Tuff Layer[J]. Engineering Failure Analysis, 2020, 117:104940.
[2]AHMED S S, IQBAL A, SARWAR R, et al. Modeling the Energy Consumption of a Lift[J]. Energy and Buildings, 2014, 71:61-67.
[3]ZHU L D, XUE P S, LAN Q, et al. Recent Research and Development Status of Laser Cladding:a Review[J]. Optics & Laser Technology, 2021, 138:106915.
[4]PEKKARINEN J, KUJANPAA V, SALMINEN A. Laser Cladding with Scanning Optics:Effect of Power Adjustment[J]. Journal of Laser Applications, 2012, 24(3):032003.
[5]王浩, 李天赐, 张乐乐. 激光熔覆技术在结构修复上的应用现状[J]. 热加工工艺, 2017, 46(22):13-17.
WANG Hao, LI Tianci, ZHANG Lele. The Application Status of Laser Cladding Technology in Structural Repair[J]. Thermal Processing Technology, 2017, 46(22):13-17.
[6]HUANG W. Study on Mould Laser Cladding Refabrication Process Based on PID[J]. Hot Working Technology, 2013, 42(14):166-168.
[7]LIU J W, WANG Y, COSTIL S, et al. Numerical and Experimental Analysis of Molten Pool Dimensions and Residual Stresses of NiCrBSi Coating Treated by Laser Post-remelting[J]. Surface and Coatings Technology, 2017, 318:341-348.
[8]LUO K Y, JING X, SHENG J, et al. Characterization and Analyses on Micro-hardness, Residual Stress and Microstructure in Laser Cladding Coating of 316L Stainless Steel Subjected to Massive LSP Treatment[J]. Journal of Alloys and Compounds, 2016, 673:158-169.
[9]DAS B, GOPINATH M, NATH A K, et al. Effect of Cooling Rate on Residual Stress and Mechanical Properties of Laser Remelted Ceramic Coating[J]. Journal of the European Ceramic Society, 2018, 38(11):3932-3944.
[10]顾建强, 骆芳, 姚建华. 激光熔覆过程残余应力的数值模拟[J]. 激光与光电子学进展, 2010, 47(10):81-86.
GU Jianqiang, LUO Fang, YAO Jianhua. Numerical Simulation of Residual Stress in Laser Cladding Process[J]. Progress in Laser and Optoelectronics, 2010, 47(10):81-86.
[11]王冬阳, 来佑彬, 杨波, 等. 工艺参数对多道搭接等离子熔覆残余应力的影响[J]. 真空, 2019, 56(6):80-84.
WANG Dongyang, LAI Youbin, YANG Bo, et al. The Influence of Process Parameters on the Residual Stress of Multi-pass Plasma Cladding[J]. Vacuum, 2019, 56(6):80-84.
[12]来佑彬, 王冬阳, 杨波, 等. 工艺参数对钴基合金等离子熔覆残余应力的影响[J]. 表面技术, 2019, 48(6):314-321.
LAI Youbin, WANG Dongyang, YANG Bo, et al. Influence of Process Parameters on Residual Stress of Cobalt-based Alloy Plasma Cladding[J]. Surface Technology, 2019, 48(6):314-321.
[13]王丽芳, 孙亚新, 朱刚贤, 等. 激光熔覆316L不锈钢残余应力工艺参数的优化模拟[J]. 应用激光, 2019, 39(3):376-380.
WANG Lifang, SUN Yaxin, ZHU Gangxian, et al. Optimal Simulation of Residual Stress Process Parameters for Laser Cladding 316L Stainless Steel[J]. Applied Laser, 2019, 39(3):376-380.
[14]傅卫, 方洪渊, 白新波, 等. 工艺路径对多层多道激光熔覆残余应力的影响[J]. 焊接学报, 2019, 40(6):29-33.
FU Wei, FANG Hongyuan, BAI Xinbo, et al. Influence of Process Path on Residual Stress of Multilayer and Multi-channel Laser Cladding[J]. Transactions of the China Welding Institution, 2019, 40(6):29-33.
[15]胡华南,陈澄洲,周泽华.剥层测量残余应力的修正[J].华南理工大学学报(自然科学版),1992, 20(4):47-57.
HU Huanan, CHEN Chengzhou, ZHOU Zehua. The Correction of the Residual Stress of the Delamination Measurement [J]. Journal of South China University of Technology (Natural Science Edition), 1992, 20(4):47-57.
[16]杜博睿, 张学军, 郭绍庆, 等. 激光快速成形GH4169合金显微组织与力学性能[J]. 材料工程, 2017, 45(1):27-32.
DU Borui, ZHANG Xuejun, GUO Shaoqing, et al. Microstructure and Mechanical Properties of Laser Rapid Forming GH4169 Alloy[J]. Materials Engineering, 2017, 45(1):27-32.
[17]WANG H Z, CHENG Y H, ZHANG X C, et al. Effect of Laser Scanning Speed on Microstructure and Properties of Fe Based Amorphous/Nanocrystalline Cladding Coatings[J]. Materials Chemistry and Physics, 2020, 250:123091.
[18]STEVENS E L, TOMAN J, TO A C, et al. Variation of Hardness, Microstructure, and Laves Phase Distribution in Direct Laser Deposited Alloy 718 Cuboids[J]. Materials & Design, 2017, 119:188-198.
[19]SUNG B P. Heterogeneous Nucleation Models to Predict Grain Size in Solidification[J]. Progress in Materials Science, 2021, 123, 100822.
[20]ZHU M L, XUAN F Z. Correlation between Microstructure, Hardness and Strength in HAZ of Dissimilar Welds of Rotor Steels[J]. Materials Science and Engineering:A, 2010, 527(16/17):4035-4042.
[21]ZHANG J, YU M J, LI Z Y, et al. The Effect of Laser Energy Density on the Microstructure, Residual Stress and Phase Composition of H13 Steel Treated by Laser Surface Melting[J]. Journal of Alloys and Compounds,2021, 856:156168.
[22]SHI BW, LI T, WANG D, et al. Investigation on Crack Behavior of Ni60A Alloy Coating Produced by Coaxial Laser Cladding[J]. Journal of Materials Science, 2021, 56(23):13323-13336.
文章导航

/

〈 〉