淬硬钢已加工表面极易产生白层,对零件的服役性能造成很大影响,采用激光加热辅助车削替代常规车削来加工淬硬钢可解决白层形成的问题。利用VDFLUX用户子程序建立了热力耦合移动激光加热辅助车削过程有限元模型并进行仿真。基于有限元模型仿真结果和白层形成临界切削速度预测模型,分析了不同激光预热参数对白层形成临界切削速度的影响。结果表明,在选用的激光预热参数范围内(激光功率P为200~600 W,激光光斑半径R为0.5~0.9 mm,激光光斑到刀尖点的距离L为5~15 mm),适当减小P和L、增大R均能增大白层形成临界切削速度的上限,在优选的激光预热参数(P=200 W,R=0.9 mm,L=5 mm)下,淬硬钢已加工表面白层形成的临界切削速度较常规切削提高了约26.09%。
It was easy to produce a white layer on the machined surfaces of hardened steels, which had a serious impact on service performance of parts. To solve the problems of white layer formation, LAT was therefore proposed to replace conventional turning for hardened steels. FEM of thermal-mechanical coupling LAT processes was established by VDFLUX user subroutine. Based on simulation results of FEM and prediction model of critical cutting speed of white layer formation, the influences of different laser preheating parameters on critical cutting speed of white layer formation were analysed. The results show that the upper limit of the critical cutting speed of white layer formation may be increased by appropriately reducing laser power, increasing laser spot radius, and shortening the distance from laser spot to tool tip within the ranges of laser preheating parameters selected, such as laser power P is as 200~600W,laser spot radius R is as 0.5~0.9 mm,distance between laser spot and tool tip L is as 5~15 mm. Under the optimized laser preheating parameters(P=200 W, R=0.9 mm, L=5 mm), the critical cutting speed of white layer formation on the machined surfaces of hardened steels is higher than that of conventional cutting to about 26.09%.
[1]GUO Y B, WARREN A W, HASHIMOTO F. The Basic Relationships between Residual Stress, White Layer, and Fatigue Life of Hard Turned and Ground Surfaces in Rolling Contact[J]. CIRP Journal of Manufacturing Science and Technology, 2010, 2(2):129-134.
[2]KOUNTANYA R, AL-ZKERI I, ALTAN T. Effect of Tool Edge Geometry and Cutting Conditions on Experimental and Simulated Chip Morphology in Orthogonal Hard Turning of 100Cr6 Steel[J]. Journal of Materials Processing Technology, 2009, 209(11):5068-5076.
[3]HOSSEINI S B, BENO T, KLEMENT U, et al. Cutting Temperatures during Hard Turning—Measurements and Effects on White Layer Formation in AISI 52100[J]. Journal of Materials Processing Technology, 2014, 214(6):1293-1300.
[4]徐颖强, 李娜娜, 李万钟,等. 硬态切削工件表面白层厚度预测方法[J]. 机械工程学报, 2015, 51(3):182-189.
XU Yingqiang, LI Nana, LI Wanzhong, et al. Prediction Method of White Layer Thickness on Hard Cutting Workpiece Surface[J]. Journal of Mechanical Engineering, 2015, 51 (3):182-189.
[5]HASSANPOUR H, SADEGHI M H, RASTI A, et al. Investigation of Surface Roughness, Microhardness and White Layer Thickness in Hard Milling of AISI 4340 Using Minimum Quantity Lubrication[J]. Journal of Cleaner Production, 2016, 120:124-134.
[6]ZHANG X M, CHEN L, DING H. Effects of Process Parameters on White Layer Formation and Morphology in Hard Turning of AISI52100 Steel[J]. Journal of Manufacturing Science Engineering, 2016, 30(7):1-6.
[7]CHOU Y K, HUI S. Tool Nose Radius Effects on Finish Hard Turning[J]. Journal of Materials Processing Technology, 2004, 148(2):259-268.
[8]ATTANASIO A, UMBRELLO D, CAPPELLINI C, et al. Tool Wear Effects on White and Dark Layer Formation in Hard Turning of AISI 52100 Steel[J]. Wear, 2012, 286/287:98-107.
[9]MIN S S, LEE C M. Determination of Optimal Laser Power According to the Tool Path Inclination Angle of a Titanium Alloy Workpiece in Laser-assisted Machining[J]. The International Journal of Advanced Manufacturing Technology, 2016, 83(9/12):1717-1724.
[10]TIAN Y, SHIN Y C. Multiscale Finite Element Modeling of Silicon Nitride Ceramics Undergoing Laser-assisted Machining[J]. Journal of Manufacturing Science Engineering, 2006, 129(2):287-295.
[11]GERMAIN G, DAL SANTO P, LEBRUN J L. Comprehension of Chip Formation in Laser Assisted Machining[J]. International Journal of Machine Tools and Manufacture, 2011, 51(3):230-238.
[12]NASR M, BALBAA M, ELGAMAL H. Modelling Machining-induced Residual Stresses after Laser-assisted Turning of Steels[J]. Advanced Materials Research, 2014, 996:622-627.
[13]LIU C, SHI Y. Modelling and Simulation of Laser Assisted Milling Process of Titanium Alloy[J]. Procedia CIRP, 2014, 24:134-139.
[14]PANJEHPOUR A, YAZDI M, SHOJA-RAZAVI R. An Experimental Investigation of Pulsed Laser-assisted Machining of AISI 52100 Steel[J]. Optics Laser Technology, 2014, 63:137-143.
[15]TADAVANI S A, RAZAVI R S, VAFAEI R. Pulsed Laser-assisted Machining of Inconel 718 Superalloy[J]. Optics & Laser Technology, 2017, 87:72-78.
[16]JOHNSON R, COOK W K. A Constitutive Model and Data for Metals Subjected to Large Strains High Strain Rates and High Temperatures.[J]. Engineering Fracture Mechanics, 1983(21):541-548.
[17]ZHANG X, WU S, WANG H, et al. Predicting the Effects of Cutting Parameters and Tool Geometry on Hard Turning Process Using Finite Element Method[J]. Journal of Manufacturing Science Engineering, 2011, 133(4).
[18]IQBAL S A, MATIVENGA P T, SHEIKH M A. An Investigative Study of the Interface Heat Transfer Coefficient for Finite Element Modelling of High-speed Machining[J]. Proceedings of the Institution of Mechanical Engineers, Part B:Journal of Engineering Manufacture, 2008, 222(11):1405-1416.
[19]张方圆. 硬切削GCr15轴承钢表面变质层微观组织及抗磨损性能研究[D]. 大连:大连理工大学, 2019.
ZHANG Fangyuan. Microstructure and Wear Resistance of Surface Modified Layer of GCr15 Bearing Steel in Hard Cutting[D]. Dalian:Dalian University of Technology, 2019.
[20]KHODABAKHSHI F, KAZEMINEZHAD M. Differential Scanning Calorimetry Study of Constrained Groove Pressed Low Carbon Steel:Recovery, Recrystallisation and Ferrite to Austenite Phase Transformation[J]. Materials Science Technology, 2014, 30(7):765-773.
[21]张小俭, 黎昊宇, 李文龙, 等. 一种金属材料对激光的吸收率的标定方法:中国, CN107462597A[P]. 2017-12-12.
ZHANG Xiaojian, LI Haoyu, LI Wenlong, et al. A Calibration Method for Laser Absorptivity of Metal Materials:China, CN107462597A[P]. 2017-12-12