先进材料加工工程

管坯大变形自由推压缩径残余应力的研究

展开
  • 1. 燕山大学车辆与能源学院,秦皇岛,066004
    2. 燕山大学机械工程学院,秦皇岛,066004
    3. 唐山学院交通与车辆工程系,唐山,063000
刘恒,男,1989年生,博士研究生。研究方向为车辆关键零部件轻量化理论与技术。E-mail:liuhenghd@163.com。

收稿日期: 2020-07-28

  网络出版日期: 2021-06-24

基金资助

河北省自然科学基金(E2016203352);河北省重大科技成果转化专项(20282202Z);河北省高等学校科学技术研究项目(QN2019335)

Study on the Residual Stress of Large Deformation Free Pushing Diameter-reducing Tube Blanks#br#

Expand
  • 1. School of Vehicle and Energy, Yanshan University, Qinhuangdao,Hebei, 066004
    2. School of Mechanical Engineering, Yanshan University, Qinhuangdao,Hebei, 066004
    3. Department of Transportation and Vehicle Engineering, Tangshan University, Tangshan, Hebei, 063000

Received date: 2020-07-28

  Online published: 2021-06-24

摘要

管坯大变形自由推压缩径时端部存在翘曲,即端部外径大于定径区外径。针对端部翘曲区进行变形分析,并基于平衡条件推导了周向残余应力与翘曲变形和剪应力的关系表达式,揭示了由内表面层到外表面层整体存在周向残余拉应力的事实。在三向液压机上进行219 mm×7.5 mm无缝钢管的双侧大变形缩径,在缩径管件上截取包含端部翘曲区和定径区的试样,在其内外表面不同区域选取测量点,并采用X射线衍射法测量残余应力,端部翘曲区测量结果与理论分析结果趋势一致。针对缩径管件变形过程,采用ABAQUS软件进行有限元模拟,缩径变形及缩径力的模拟结果与缩径试验结果吻合,内外表面层残余应力的模拟结果与X射线衍射法测量结果趋势一致。给出了自定径区至端部沿壁厚方向及沿轴向方向的残余应力分布规律。

本文引用格式

刘恒, 王连东, 王晓迪, 刘超, . 管坯大变形自由推压缩径残余应力的研究[J]. 中国机械工程, 2021 , 32(11) : 1354 -1360 . DOI: 10.3969/j.issn.1004-132X.2021.11.012

Abstract

The ends of large deformation free pushing diameter-reducing tube blanks were warped, that is, the outer diameters of the ends were larger than that of the sizing areas. For the end warpage areas, based on the deformation analysis and mechanics equilibrium conditions, the formula of circumferential residual stress was deduced from the warpage deformations and shear stress. It is revealed that the circumferential residual stress is characterized as tensile stress from the inner to outer surface. The double-sided large deformation diameter-reducing of 219 mm × 7.5 mm seamless steel pipes were carried out on the three-dimentional hydraulic press. With the diameter-reducing sample intercepted, the measuring points were selected in the inner and outer surfaces of the end warpage areas and sizing areas, and the residual stress was measured by X-ray diffraction method. The trend of end warpage area measurements were consistent with the theoretical analysis. For the diameter-reducing processes, the finite element simulation was carried out with ABAQUS software, the results of the deformation and force are in good agreement with the diameter-reducing experiments, and the results of residual stress in the inner and outer surfaces are consistent with the X-ray measurement. Furthermore, the distribution laws of residual stress along the wall thickness direction and the axial direction from the sizing areas to the end are revealed respectively.

参考文献

[1]FISHER W P, DAY A J. A Study of the Factors Controlling the Tube-sinking Process for Polymer Materials[J]. Journal of Materials Processing Technology, 1997, 68: 156-162.
[2]滕宏春, 林桂霞, 胡平. 带有动芯轴的管料壁厚减薄缩口成形的理论解析[J]. 机械工程学报, 2005, 41(7): 234-238.
TENG Hongchun, LIN Guixia, HU Ping. Theoretical Analysis and Experiment of Sinking of Tube with a Moving Mandrel[J]. Journal of Mechanical Engineering, 2005, 41(7): 234-238.
[3]SALEHI J, REZAEIAN A, TOROGHINEJAD M R. Fabrication and Characterization of a Bimetallic Al/Cu Tube Using the Tube Sinking Process[J]. International Journal of Advanced Manufacturing Technology, 2018, 96(1/4): 153-159.
[4]王连东.回转壳体正负成形理论及汽车桥壳胀形工艺的研究[D]. 秦皇岛: 燕山大学, 2001.
WANG Liandong. Study on Positive-negative Forming Theory of Revolving Shell and Bulging Technology of Automobile Axle Housings[D]. Qinhuangdao: Yanshan University, 2001.
[5]ZHAO D W, DU H J, WANG G J, et al. An Analytical Solution for Tube Sinking by Strain Rate Vector Inn-erproduct Integration[J]. Journal of Materials Processing Technology, 2009, 209: 408-415.
[6]SADOK L, KUSIAK J, PACKO M, et al. State of Strain in the Tube Sinking Process[J]. Journal of Materials Processing Technology, 1996, 60(1/4): 161-166.
[7]HIRSCH T K, SILVA R A, MENEZES N R. Characterization of Local Residual Stress Inhomogeneities in Combined Wire Drawing Processes of AISI 1045 Steel Bars[J]. International Journal of Advanced Manufacturing Technology, 2014, 70(1/4): 661-668.
[8]GATTMAH J, OZTURK F, ORHAN S. Experimental and Finite Element Analysis of Residual Stresses in Cold Tube Drawing Process with a Fixed Mandrel for AISI 1010 Steel Tube[J]. International Journal of Advanced Manufacturing Technology, 2017, 93(1/4): 1229-1241.
[9]VOLLERT F, LUCHINER M, SCHUSTER S, et al. Experimental and Numerical Analyses of Residual Stresses Induced by Tube Drawing[J]. Journal of Strain Analysis for Engineering Design, 2018, 53(5): 364-375.
[10]王连东, 赵石岩, 高鹏飞, 等. 管坯推压缩径端部翘曲机理及其影响因素分析[J]. 塑性工程学报, 2005, 12(3): 76-79.
WANG Liandong, ZHAO Shiyan, GAO Pengfei, et al. Analysis of Buckling in Push-sinking and Its Influence Factor[J]. Journal of Plasticity Engineering, 2005, 12(3): 76-79.
[11]王连东, 刘超, 刘恒, 等. 芯轴外径对大变形推压-拉拔复合缩径的影响[J]. 中国机械工程, 2018, 29(17): 2131-2136.
WANG Liandong, LIU Chao, LIU Heng, et al. Effects of Mandrel Diameters on Large Deformation Pushing-pulling Necking[J]. China Mechanical Engineering, 2018, 29(17): 2131-2136.
[12]LIU G H, GUO Y Q, JIANG Z. Influence ofHeating Models on Necking Deformation during Tube Extrusion Process[J]. Advanced Materials Research, 2011, 189/193: 1778-1781.
[13]吴娜, 王连东, 沈亚坤, 等. 充液压制成形汽车桥壳后盖区开裂分析及预成形管坯形状优化设计[J]. 中国机械工程, 2016, 27(23): 3246-3251.
WU Na, WANG Liandong, SHEN Yakun, et al. Cracking Analysis of Rear Covers and Shape Optimization of Preformed Pipes for Filling-pressing Forming Axle Housings[J]. China Mechanical Engineering, 2016, 27(23): 3246-3251.
[14]高玉魁. 残余应力基础理论及应用[M]. 上海: 上海科学技术出版社, 2019.
GAO Yukui. Theory and Application of Residual Stresses[M]. Shanghai: Shanghai Scientific & Technical Publishers, 2019.
[15]胡永会, 吴运新, 陈磊, 等. X 射线法测量淬火铝合金厚板表面残余应力[J]. 中国材料进展, 2011, 30(2): 51-54.
HU Yonghui, WU Yunxin, CHEN Lei, et al. Experimental Measurement of Surface Residual Stresses of Quenched Aluminum Alloy Thick Plate by X-Ray Method[J]. Materials China, 2011, 30(2): 51-54.
[16]朱刚, 张晖, 张旺峰, 等. 高强度钛合金管材残余应力测试及对比分析[J]. 稀有金属材料与工程, 2014, 43(10): 2492-2496.
ZHU Gang, ZHANG Hui, ZHANG Wangfeng, et al. Test and Analysis of the Residual Stress in Ti-3Al-2.5V Tubes with Different Processes[J]. Rare Metal Materials and Engineering, 2014, 43(10): 2492-2496.
文章导航

/

〈 〉