为实现多层金刚石磨粒逐层激光钎焊成形,从单道扫描到单层扫描,再到多层扫描,系统研究了镍铬合金与金刚石磨粒的多层激光钎焊工艺。通过提取钎焊道与层的截面成形特征参量,对钎焊层截面成形质量进行参数化评价,并结合钎焊层表面形态,对钎焊层综合成形特性进行评价和讨论,研究了工艺参数对钎焊成形的影响。研究结果表明:激光功率与扫描速度是影响钎焊成形的重要因素,不仅影响着合金粉末的熔合程度、熔池宽度,还影响金刚石的分散状态和钎料对金刚石的浸润包裹性,最终影响钎焊层的平整性。当道与道之间的搭接率为30%~40%时,钎焊成形质量较好。在采用逆向扫描策略,扫描道数为10、固定激光功率为700 W、扫描速度为15 mm/s、光斑直径为1.5 mm、搭接率为30%的条件下,实现了多层磨粒的激光逐层钎焊成形,钎料对金刚石浸润包裹充分,钎焊层中间区域平整连续,整体成形质量好。
In order to realize the layer-by-layer laser brazing of multilayer diamond abrasive particles, the multilayer laser brazing process of Ni-Cr alloy and diamond abrasive particles was studied systematically, from single channel scanning to single layer scanning and then to multilayer scanning. The brazing channel and layer of cross section shape characteristic parameters were extracted, the brazing layer section forming parameterized evaluations was carried out. Combined with the brazing layer surface morphology, the brazing layer composite forming characteristics was evaluated and discussed, the influence of brazing process parameters on forming was studied. The results show that the laser power and scanning speed are the important factors affecting brazing forming. They affect the degree of fusion of alloy powders, molten pool width, and further affect the dispersion state of diamond and performance that diamonds are infiltrated and wrapped by solders, finally affect the smoothness of the brazing layers. When the overlapping rate between channels is as 30%~40%, the brazing forming quality is better. In the reverse scanning strategy, the number of scanning channels is as 10, the fixed laser power is as 700 W, the scanning speed is as 15 mm/s, the spot diameter is as 1.5 mm, the overlapping rate is as 30%, the laser brazing of multilayer abrasives is realized, the filler metal to the diamond infiltration package is sufficient, the middle area of the brazing layer is smooth and continuous, the overall forming quality is good.
[1]DU Q, WANG X, ZHANG S, et al. Research Status on Surface Metallization of Diamond[J].Materials Research Express, 2019, 6(12):122005.
[2]DING W F, XU J H, CHEN Z Z, et al. Fabrication and Performance of Porous Metal-bonded CBN Grinding Wheels Using Alumina Bubble Particles as Pore-forming Agents[J]. International Journal of Advanced Manufacturing Technology, 2013, 67:1309-1315.
[3]DENKENA B, GROVE T, BREMER I, et al. Design of Bronze-bonded Grinding Wheel Properties[J]. CIRP Annals—Manufacturing Technology, 2016, 65(1):333-336.
[4]YADAV A, JOSHI J, SINGH D K, et al. Development of Laser Beam Welding for the Lip Seal Configuration[J]. Fusion Engineering & Design, 2015, 96/97:192-198.
[5]PABLOS-MARTIN A D, BENNDORF G, TISMER S, et al.Laser-welded Fused Silica Substrates Using a Luminescent Fresnoite-based Sealant[J]. Optics & Laser Technology, 2016, 80:176-185.
[6]LEE K J, KUMAI S, ARAI T. Interfacial Microstructure and Strength of Steel to Aluminum Alloy Lap Joints Welded by a Defocused Laser Beam[J].Materials Transactions, 2005, 46(8):1847-1856.
[7]李时春, 周振红, 伍俏平, 等. 激光钎焊制备金属结合剂金刚石砂轮研究进展[J]. 兵器材料科学与工程, 2019, 42(2):111-120.
LI Shichun, ZHOU Zhenhong, WU Qiaoping,et al. Research Progress on Preparation of Metal Bond Diamond Grinding Wheel by Laser Brazing[J]. Ordnance Materials Science and Engineering, 2019, 42(2):111-120.
[8]HUANG S F, TSAI H L, LIN S T. Laser Brazing of Diamond Grits Using a Cu-15Ti-10Sn Brazing Alloy[J]. Materials Transactions, 2002, 43(10):2604-2608.
[9]杨卫红, 唐霞辉, 秦应雄,等. 高功率CO2激光钎焊金刚石颗粒[J]. 中国激光, 2007, 34(4):569-573.
YANG Weihong, TANG Xiahui, QING Yingxiong, et al. High Power CO2 Laser Brazing of Diamond Grits[J]. Chinese Journal of Lasers, 2007, 34(4):569-573.
[10]杨志波, 徐九华, 傅玉灿,等. 钢基体上镍基钎料
激光钎焊金刚石磨粒的界面结构[J]. 机械工程材料, 2007, 31(5):17-19.
YANG Zhibo, XU Jiuhua, FU Yucan, et al. Interface Structure of Laser Brazed Diamond Abrasive Grains on Nickel-based Brazing Filler Metal on Steel Substrate[J]. Materials for Mechanical Engineering, 2007, 31(5):17-19.
[11]杨志波, 徐九华, 刘爱菊. 激光钎焊金刚石磨粒界面微结构分析[J]. 焊接学报, 2010, 31(10):9-12.
YANG Zhibo, XU Jiuhua, LIU Aiju. InterfacialMicrostructure Analysis of Laser Brazed Diamond Abrasive[J]. Transactions of the China Welding Institution, 2010, 31(10):9-12.
[12]YANG L J, LI B, YAO J H, ea al. Effects of Diamond Size on the Deposition Characteristic and Tribological Behavior of Diamond/Ni60 Composite Coating Prepared by Supersonic Laser Deposition[J]. Diamond & Related Materials, 2015, 58:139-148.
[13]ROMMEL D, SCHERM F, KUTTNER C, et al. Laser Cladding of Diamond Tools:Interfacial Reactions of Diamond and Molten Metal[J]. Surface & Coatings Technology, 2016, 291:62-69.
[14]YANG Z B, ZHANG M J, ZHANG Z, et al. AStudy on Diamond Grinding Wheels with Regular Grain Distribution Using Additive Manufacturing (AM) Technology[J]. Materials & Design, 2016, 104:292-297.
[15]YANG Z B, LIU A J, YANG R Y, et al. Interface Microstructure and Formation Mechanism of Diamond Abrasives Laser Brazed with Ni-Cr Solder[J]. Rare Metal Materials & Engineering, 2016, 45(5):1152-1156.
[16]TIAN C C, LI X K, ZHANG S B, et al. Study on Design and Performance of Metal-bonded Diamond Grinding Wheels Fabricated by Selective Laser Melting (SLM)[J]. Materials & Design, 2018, 156:52-61.
[17]张洋, 宋博瀚, 薛峰. 稀释率对镍基合金激光熔覆层组织和性能的影响 [J]. 应用激光, 2016, 36(3):259-264.
ZHANG Yang, SONG Bohan, XUE Feng. Effect of Dilution Rate on Microstructure and Properties of Nickel Base Alloy Laser Cladding Layer[J]. Applied Laser, 2016, 36(3):259-264.