Aiming at the defects such as pores, microcracks, loose surface structure, poor continuity and poor surface quality in the ESD layer, a machining method of “ESD-remelting and rolling” was proposed herein. Taking the conventional ESD as a comparison,experiments were carried out using the new method. The deposited layers were analyzed. The results show that during the remelting and rolling processes, the electrode has a large extrusion and rolling effects on the deposition surfaces. Remelting and rolling dressing may effectively eliminate defects such as pores, microcracks and loose tissue inside the sediment layer. In addition, such process may refine the grain and improve the continuity and integrity of the layers. It is believed that the rotating electrode has a significant grinding coating effectiveness on the surfaces of the deposited layers. The defects such as surface micropores and cracks are basically eliminated, experimental results show that the roughness values of the remelting and rolling coating is 76.3% of the conventional ESD coating, which indicate the surface quality of the deposited layers is improved.
[1] 刘志东.特种加工[M].北京:北京大学出版社,2013:12-16,67. LIU Zhidong. Special Machining[M].Beijing:Peking University Press, 2013:12-16,67.
[2] 高玉新, 赵程, 易剑. 粉末预置法电火花沉积WC-8Co涂层分析[J]. 焊接学报, 2012,33(3):49-52. GAO Yuxin, ZHAO Cheng, YI Jian. Analysis on WC-8Co Electro-spark Deposition Coating with Powder Presetting Method[J]. Transactions of the China Welding Institution, 2012,33(3):49-52.
[3] 金柏冬, 曹国辉, 王振龙,等. 空气中微细电火花沉积的工艺规律研究[J]. 中国机械工程, 2006, 17(2):111-115. JIN Baidong, CAO Guohui, WANG Zhenlong, et al. Research on Processing Law of Micro-EDD in Air[J]. China Mechanical Engineering, 2006, 17(2):111-115.
[4] WANG Haibo, WANG Shirong, YU Chunbo. Surface Modification of (Tb, Dy) Fe2 Alloy by Nitrogen Ion Implantation[J]. Rare Materials:English Version, 2011, 29(9):878-882.
[5] 赵运才, 刘宗阳, 杨雷雷. 弧比变化对电火花沉积Ni201修复层界面行为的影响[J]. 中国机械工程, 2016, 27(10):1399-1403. ZHAO Yuncai, LIU Zongyang, YANG Leilei. Effects of Different Arc Rates on Interface Behavior of Ni201 Repaired Layers by Electro-spark Deposition[J]. China Mechanical Engineering, 2016, 27(10):1399-1403.
[6] ZENG Chao, TIAN Wei, HUA Liang. A Comprehensive Study of Thermal Damage Consequent to Laser Surface Treatment[J]. Materials Science & Engineering, 2013, 64(6):381-388.
[7] 汪瑞军, 程家龙, 黄小鸥,等. 电火花表面强化过程中的"阳极粘连"现象[J]. 焊接, 2005(8):37-40. WANG Ruijun, CHENG Jialong, HUANG Xiaoou, et al. Phenomena of a Node-conglutinating in the Course of Electrospark Surface Streng Thening[J].Welding & Joining,2005(8):37-40.
[8] 汪瑞军, 常志龙, 钱乙余,等. 电火花强化过程中两极间质量过渡规律[J]. 焊接, 2004(11):21-24. WANG Ruijun, CHANG Zhilong, QIAN Yiyu, et al. Mass Transfer Regularity between the Two Electrodes in Course of Electrospark Surface Strengthening[J]. Welding & Joining, 2004(11):21-24.
[9] 何鹏, 吴承东, 钱乙余, 等. 钛合金表面电火花沉积WC电极的粘连行为分析[J]. 焊接学报, 2006,27(4):25-28. HE Peng, WU Chengdong, QIAN Yiyu, et al. Adhesion Behavior of WC Coating Deposited on Titanium Alloy by Electrospark Deposition[J]. Transactions of the China Welding Institution, 2006,27(4):25-28.
[10] 王令双, 曹国剑, 马欣新,等. GH4169表面电火花沉积NiCrAlY涂层的制备[J]. 焊接学报, 2017,38(7):104-108. WANG Lingshuang, CAO Guojian, MA Xinxin, et al. Preparation of NiCrAlY Coating Electro-spark Deposited on GH4169 Alloy[J]. Transactions of the China Welding Institution, 2017,38(7):104-108.
[11] 李福海, 代明江, 陈兴驰,等. H13模具钢表面电火花沉积层工艺及其性能研究[J]. 材料研究与应用, 2018,12(1):22-27. LI Fuhai, DAI Mingjiang, CHENG Xingchi, et al. Study on the Process and Properties of Electrical Discharging Deposition on H13 Steel[J]. Materials Research and Application, 2018,12(1):22-27.
[12] 魏国. 电火花沉积层质量的影响因素研究[J]. 电加工与模具, 2016(6):56-59. WEI Guo. Study on Factors Affecting of Electrospark Deposition Layer Quality[J]. Electromachining & Mould, 2016(6):56-59.
[13] 倪杨, 郭常宁, 薛锐. 放电通道振荡特性分析及其蚀除机理的研究[J]. 电加工与模具, 2009(1):9-12. NI Yang, GUO Changning, XUE Rui. Analysis of the Plasma Oscillation and Erosion Mechanish in Electrical Discharge Channel[J]. Electromachining & Mould, 2009(1):9-12.
[14] 朱凯, 王春梅, 张怡茹,等. 微细电火花放电通道扩展的研究[J]. 电加工与模具, 2015(3):21-25. ZHU Kai, WANG Chunmei, ZHANG Yiru, et al. Study on Expansion of Micro-EDM Discharge Channel[J]. Electromachining & Mould, 2015(3):21-25.
[15] 韩红彪, 郭敬迪, 焦文清. 旋转电极电火花沉积/堆焊的放电机理[J]. 焊接学报, 2019,40(5):67-72. HAN Hongbiao, GUO Jingdi, JIAO Wenqing. Discharge mechanism of Electro-spark Deposition with Rotary Electrode[J]. Transactions of the China Welding Institution, 2019,40(5):67-72.
[16] 杨飞, 杨蛟, 华晗, 等. 放电能量实时控制的双极性电火花加工脉冲电源[J]. 电加工与模具, 2017(6):1-5. YANG Fei, YANG Jiao, HUA Han,et al. Bipolar Pulse Power Generator for EDM with Real-time Discharge Energy Control[J]. Electromachining & Mould, 2017(6):1-5.
[17] SINGH J,SHARMA R K. Green EDM Strategies to Minimize Environmental Impact and Improve Process Efficiency[J].Journal for Manufacturing Science and Production,2016,16(4):273-290.
[18] 朱胜, 袁鑫鹏, 徐安阳,等. QAl9-4铜合金表面电火花沉积试验研究[J]. 热加工工艺, 2017(8):143-147. ZHU Sheng, YUAN Xinpeng, XU Anyang, et al. Electro-spark Deposition Experiment on Surface of QAl9-4 Copper Alloy[J].Hot Working Technology, 2017(8):143-147.