测试了CoCrMo合金表面沉积类金刚石薄膜与CoCrMo在水溶液润滑下的摩擦磨损行为。结果表明:摩擦副在不同浓度牛血清白蛋白溶液润滑下的平均摩擦因数均在0.10左右,CoCrMo合金销磨损量最小值为1.69×10-5 mm3;相同条件下,生理盐水溶液润滑的磨损量为1.38×10-5 mm3,且销表面有转移膜生成;牛血清白蛋白溶液润滑时,界面蛋白吸附层屏蔽了转移膜的形成。根据结果可知,转移膜的形成经历了磨屑附着、连续转移、局部脱落的过程。
Tribological behavior of the DLC films was analyzed systematically, which were deposited on the polished surfaces of CoCrMo alloy with respect to the CoCrMo under the lubrication of aqueous solution. Results show that the average friction coefficient is about 0.10 under bovine serum albumin (BSA) solution lubrication with different concentrations,and the smallest wear loss of CoCrMo pin is about 1.69×10-5 mm3. In the same conditions, the wear loss of CoCrMo pins under the lubrication of physiological saline solution is 1.38×10-5 mm3. The DLC transfer layer exists on the wear scar lubricated with physiological saline solution. It indicates that the formation of DLC transfer layer is inhibited by the adsorption of bovine serum albumin protein layer. The formation of transfer layer has undergone the processes of wear debris adhesion, continuous transferring, and partial delamination.
[1] HAERI M, GILBERT J L. Study of Cellular Dynamics on Polarized CoCrMo Alloy Using Time-lapse Live-cell Imaging[J]. Acta Biomaterialia, 2013, 9(11):9220-9228.
[2] 席翔, 夏延秋, 曹正锋, 等. 高速电弧喷涂Al-Ni-Mm-Co涂层在脂润滑下的摩擦磨损性能[J]. 中国机械工程, 2017, 28(2):215-222. XI Xiang, XIA Yanqiu, CAO Zhengfeng, et al. Tribology Performance of High Speed Arc Spraying Al-Ni-M-Co Film under Lubrication Condition of Different Greases[J]. China Mechanical Engineering, 2017, 28(2):215-222.
[3] BALAGNA C, AGA M G, SPRIANO S. Tantalum-based Multilayer Film on Cobalt Alloys in Total Hip and Knee Replacement[J]. Materials Science and Engineering C, 2012, 32(4):887-895.
[4] LIU H, LENG Y, TANG J, et al. Tribological Performance of Ultra-high-molecular-weight Polyethylene Sliding against DLC-coated and Nitrogen Ion Implanted CoCrMo Alloy Measured in a Hip Joint Simulator[J]. Surface and Coatings Technology, 2012, 206(23):4907-4914.
[5] GALETZ M C, SEIFERTH S H, THEILE B, et al. Potential for Adhesive Wear in Friction Couples of UHMWPE Running against Oxidized Zirconium, Titanium Nitride Films, and Cobalt-chromium Alloys[J]. Journal of Biomedical Materials Ressearch, 2010, 93B(2):468-475.
[6] VITU T, ESCUDEIRO A, Polcar T, et al. Sliding Properties of Zr-DLC Film:the Effect of Tribolayer Formation[J]. Surface & Film Technology, 2014, 258:734-745.
[7] CHO Y K, JANG W S, YOO S, et al. Synthesis of Conductive Ti-C:H Films on the Stainless Steel Plates by PECVD Process[J]. Surface & Films Technology, 2008, 202(22/23):5390-5394.
[8] VENGUDUSAMY B, GRAFL A, PREINFALK K. Tribological Properties of Hydrogenated Amorphous Carbon under Dry and Lubricated Conditions[J]. Diamond & Related Materials, 2014, 41:53-64.
[9] SUTTON D C, LIMBERT G, STEWART D, et al. The Friction of Diamond-like Carbon Films in a Water Environment[J]. Friction, 2013, 1(3):210-221.
[10] DUONG C T, LEE J H, CHO Y, et al. Effect of Protein Concentrations of Bovine Serum Albumin and γ-globulin on the Frictional Response of a Cobalt-chromium Femoral Head[J]. Journal of Materials Science Materials in Medicine, 2012, 23(5):1323-1330.
[11] LAUX K A, SCHWARTZ C J. Influence of Linear Reciprocating and Multi-directional Sliding on PEEK Wear Performance and Transfer Film Formation[J]. Wear, 2013, 301:727-734.