Property of Electromagnetic Welded Joints of 5052 Aluminum Alloy and HC420LA High Strength Steel in Salt Fog Corrosion

  • XU Bing ,
  • OU Hang ,
  • LIU Quanxiaoxiao ,
  • XU Zhidan ,
  • LI Guangyao ,
  • CUI Junjia
Expand
  • 1. State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, Changsha, 410082;
    2. Collaborative Innovation Center of Intelligent New Energy Vehicle, Tongji University, Shanghai, 201804;
    2. SAIC-GM-WULING Automobile Co., Ltd., Liuzhou, Guangxi, 545000

Received date: 2017-10-18

  Revised date: 2018-03-18

  Online published: 2020-07-09

摘要

对5052铝合金-HC420LA高强钢的磁脉冲焊接接头进行了盐雾腐蚀试验,揭示了磁脉冲焊接接头的腐蚀机理。研究结果表明,铝-钢磁脉冲焊接接头的力学性能在盐雾腐蚀环境中的退化较为明显,腐蚀首先从焊缝两侧尖端开始,当腐蚀时间达到48h时,焊接接头强度已下降为原来的20%。断口微观分析表明,钢较低的电化学电位加快了腐蚀,接头的腐蚀行为具有自催化作用。

本文引用格式

许冰 , 欧航 , 柳泉潇潇 , 徐志丹 , 李光耀 , 崔俊佳 . 铝合金-HC420LA高强钢磁脉冲焊接接头盐雾腐蚀性能[J]. 中国机械工程, 2019 , 30(12) : 1506 -1511 . DOI: 10.3969/j.issn.1004-132X.2019.12.019

Abstract

The salt fog corrosion tests of magnetic pulse welded joints of 5052 aluminum alloy and HC420LA high strength steel were conducted, and the corrosion mechanism of magnetic pulse welded joints was revealed. The research results show that the degradation of mechanical properties of welded joints under salt fog environments is very obvious, and the corrosion starts from the first weld tip. Welded joint remained 20% strength when the corrosion time comes to 48 h. Microstructure analysis of the fracture presents that the low potential of steel accelerates the corrosion rate, and the corrosion of welded joints has self-catalysis.

参考文献

[1] MILLER W, ZHUANG L, BOTTEMA J, et al. Recent Development in Aluminum Alloys for the Automotive Industry[J]. Materials Science and Engineering A, 2000, 280(1):37-49.
[2] HAHN O, KURZOK J, TIMMERMANN R, et al. Joining of Mixed Material Constructions[EB/OL].[2016-03-22]. http://www.lwf-paderborn.de/publikationen/tagungsbaende/details-tagungsbaende/artikel//chinese-german-ultralight-symposium.
[3] 陈树君, 夏羽, 于洋, 等.异质金属材料磁脉冲焊接技术[J].航空精密制造技术,2011,47(4):33-35. CHEN Shujun, XIA Yu, YU Yang, et al. Dissimilar Metal Material Technology on Magnetic Pulse Welding[J]. Aviation Precision Manufacturing Technology, 2011, 47(4):33-35.
[4] XU Zhidan, CUI Junjia, YU Haiping, et al. Research on the Impact Velocity of Magnetic Impulse Welding of Pipe Fitting[J]. Materials and Design, 2013, 49:736-745.
[5] CUI Junjia, SUN Guangyong, LI Guangyao, et al. Specific Wave Interface and Its Formation during Magnetic Pulse Welding[J]. Applied Physics Letters, 2014, 105:221901-221904.
[6] CUI Junjia, SUN Guangyong, XU Zhidan, et al. A Study on the Critical Wall Thickness of the Inner Tube for Magnetic Pulse Welding of Tubular Al-Fe Parts[J]. Journal of Materials Processing Technology, 2016, 227:138-145.
[7] WLOKA J, LAUKANT H, GLATZEL U, et al. Corrosion Properties of Laser Beam Joints of Aluminum with Zinc-coated Steel[J]. Corrosion Science, 2007, 49(11):4243-4258.
[8] SHI Yu, LI Jie, ZHANG Gang, et al. Corrosion Behavior of Aluminum-steel Weld-brazing Joint[J]. Journal of Materials Engineering and Performance, 2016, 25(5):1916-1923.
[9] 顾玉芬, 李杰, 石玗, 等. 铝/钢异种金属电弧熔钎焊焊接接头的腐蚀性能[J]. 中国有色金属学报, 2016, 26(4):758-765. GU Yufen, LI Jie, SHI Yu, et al. Corrosion Property of Arc Welding Brazed Joint between Aluminum and Steel[J]. The Chinese Journal of Nonferrous Metals, 2016, 26(4):758-765.
[10] 于海平, 徐殿国, 李春峰. 异种金属磁脉冲连接技术的研究与应用[J]. 锻压技术,2009, 34(2):1-6. YU Haiping, XU Dianguo, LI Chunfeng. Research and Application of Magnetic Pulse Joining for Dissimilar Metal Materials[J]. Forging and Stamping Technology,2009,34(2):1-6.
[11] 崔俊佳, 袁伟, 李光耀. 汽车车身异种金属板件磁脉冲焊接工艺研究[J]. 汽车工程, 2017, 39(1):113-120. CUI Junjia, YUAN Wei, LI Guangyao.A Study on Magnetic Pulse Welding Process for Dissimilar Sheet Metals of Autobodyl[J]. Automotive Engineering, 2017, 39(1):113-120.
[12] 韩顺昌. 金属腐蚀显微组织图谱[M].北京:国防工业出版社,2008:46-47. HAN Shunchang. Atlas of Microstructure on Metal Corrosion[M].Beijing:National Defend Industry Press, 2008:46-47.
[13] 龚敏.金属腐蚀理论及腐蚀控制[M].北京:化学工业出版社,2009:113.
文章导航

/

〈 〉