通过有限元法建立了管道直流磁化的三维模型,分析了励磁状态下铁磁材料的磁特性、缺陷附近材料的磁导率分布特征以及励磁强度、管道厚度、缺陷深度对磁导率分布的影响。结果表明,饱和磁化后缺陷区域的磁导率分布并不均匀,励磁作用下内壁缺陷可引起外表面磁导率的改变,从而揭示了铁磁性管道内部缺陷检出机理,拓展了涡流检测方法的应用范围。
A 3D model of DC magnetization pipes was built with finite element method.Meanwhile the ferromagnetic material magnetic properties and the distribution of magnetic permeability around defect areas were analyzed. The effects of magnetization intensity, the thicknesses of the pipes and the depths of the flaws on magnetic permeability distribution were studied.The results show that the magnetic permeability of the defect areas is uneven distributed while saturation magnetized, and the internal defects may even cause the magnetic permeability of exterior surface changing under magnetization. The mechanism of internal defects on the ferromagnetic pipes is revealed, and the applications of the eddy current testing method are expanded.
[1] 康宜华,武新军.数字化磁性无损检测技术[M].北京:机械工业出版社, 2006. KANG Yihua, WU Xinjun.Digital Magnetic Nondestructive Testing Technology[M]. Beijing:China Machine Press, 2006.
[2] 任吉林.电磁检测[M].北京:科学出版社, 2001:64-67. REN Jilin. Electromagnetic Testing[M]. Beijing:Science Press, 2001:64-67.
[3] LEE H J, CHAN H C, MIN W N, et al. Eddy Current Testing of Type-439 Stainless Steel Tubin Gusing Magnetic Saturation Technique[J]. Journal of Mechanical Science and Technology. 2012,26(7):2081-2085.
[4] 林俊明,赖传理,任吉林.钢管涡流探伤中缺陷信号得相位分辨[J].无损检测, 2011, 33(1):2-8. LIN Junming, LAI Chuanli, REN Jilin. Phase Distinction in Eddy Current Testing for Steel Tubes[J]. Nondestructive Testing, 2011, 33(1):2-8.
[5] 熊龙辉,王平.高速漏磁检测中钢轨磁化强度的研究[J].无损检测, 2013(11):2-6. XIONG Longhui, WANG Ping.Research on Magnetization of Rail in High-speed Magnetic Flux Leakage Testing[J].Nondestructive Testing, 2013(11):2-6.
[6] 杨理践,张森林,高松巍.钢板厚度对漏磁检测效果的影响[J].无损检测, 2013(10):10-13. YANG Lijian, ZHANG Senlin, GAO Songwei. Impact of Sheet Thickness on Magnetic Flux Leakage Inspection[J]. Nondestructive Testing, 2013(10):10-13.
[7] JARVIS R, CAWLEY P, NAGY P B. Current Deflection NDE for the Inspection and Monitoring of Pipes[J].NDT&E International, 2016, 81:46-59.
[8] SURESH V, ABUDHAHIR A, DANIEL J. Development of Magnetic Flux Leakage Measuring System for Detection of Defect in Small Diameter Steam Generator Tube[J]. Measurement. 2017, 95:273-279.
[9] 史荣,王雷,王劲东,等.钢丝绳弱磁探伤数值模拟及实验研究[J].中国机械工程, 2013, 24(22):30413044. SHI Rong, WANG Lei, WANG Jindong, et al.Value Simulation and Experimental Study of a Rope Weak Magnetic Flaw Detection[J]. China Mechanical Engineering, 2013, 24(22):3041-3044.
[10] 冯搏,伍剑波,杨芸,等.钢管纵向伤高速高精漏磁探伤磁化方法[J].中国机械工程, 2014, 25(6):736740. FENG Bo, WU Jianbo, YANG Yun, et al.Research on Magnetization Method for High Speed Precision Magnetic Flux Leakage Testing of Longitudinal Defects in Speed Pipes[J].China Mechanical Engineering.2014, 25(6):736-740.
[11] 宋凯,陈超,康宜华,等.钢管内壁缺陷涡流检测的机理研究[J].失效分析与预防, 2012, 7(3):180-183. SONG Kai,CHEN Chao,KANG Yihua,et al. Study on Mechanism of Eddy Current Testing for Inner Defect of Steel Pipe[J].Failure Analysis and Prevention, 2012, 7(3):180-183.