Microstructure and properties of plasma arc additive repairing depositions for the worn rotor journal of power station equipment

  • GUO Yang ,
  • ZHANG Jianxun ,
  • XIONG Jiankun ,
  • LIU Yan ,
  • ZHAO Pengfei
Expand
  • 1. State Key Laboratory for Mechanical Behavior of Materials, Xi’An Jiaotong University, Xi’an, 710049, China;
    2. State Key Laboratory of Long-Life High Temperature Materials, Dongfang Electric Corporation Dongfang Turbine Co.,Ltd., Deyang, 618000, China

Received date: 2020-02-01

  Online published: 2021-01-12

Abstract

In view of the in situ repairing requirements of rotor journal of power plant equipment, a non preheating single-layer and multi-passes additive depositing 316L alloy was achieved on 20Cr2NiMo steel by Micro Plasma Arc Depositing process. The microstructure, hardness, chemical composition and mechanical properties of deposition and heat affected zone were analyzed. The results show that the deposition is metallurgical bonded with the substrate, and there is no crack in the cladding layer and heat affected zone; the microstructure of 316L deposition consists of austenite + δ ferrite, and the primary heat affected zone can be divided into decarburization zone, coarse-grained zone, fine-grained zone and mixed crystalline zone, and the primary coarse-grained zone is coarsened, refined and softened due to the secondary heat cycle. The difference of hardness between 316L deposition and substrate is small, while the hardness of primary coarse-grained zone is the highest, but that of secondary coarse-grained zone below 476HV0.3, and the width of heat affected zone is about 2.5 mm; the shear strength of heat affected zone is higher than that of substrate, but the plasticity of substrate is better.

Cite this article

GUO Yang , ZHANG Jianxun , XIONG Jiankun , LIU Yan , ZHAO Pengfei . Microstructure and properties of plasma arc additive repairing depositions for the worn rotor journal of power station equipment[J]. Transactions of The China Welding Institution, 2020 , 41(10) : 47 -53 . DOI: 10.12073/j.hjxb.20200201001

References

[1] 叶荣学, 孙伟, 张艾萍, 等. 滑动轴承油膜厚度变化对汽轮机转子稳定性的影响[C]//第九届全国振动理论及应用学术会议, 2017: 1062-1067.
Ye Rongxue, Sun Wei, Zhang Aiping, et al. The influence of oil film thickness of sliding bearing on the stability of steam turbine rotor[C]//The 9th National Conference on Vibration Theory and Application, 2017: 1062-1067.
[2] Shchurova A V. Modeling the turbine rotor journal restoration located on cylindrical surface of the supporting bearer[J]. Procedia Engineering, 2017, 206: 1142 - 1147.
[3] 赵景辉. 汽轮机转子轴颈划伤处理[J]. 电力安全技术, 2015(2): 10 - 11
Zhao Jinghui. Treatment of turbine rotor journal scratch[J]. Electric Safety Technology, 2015(2): 10 - 11
[4] 何新有. 汽轮机转子轴颈损伤原因分析及修复措施[J]. 发电设备, 2009, 23(3): 170 - 172
He Xinyou. Cause analysis of turbine rotor’s shaft neck damage and the repair[J]. Power Equipment, 2009, 23(3): 170 - 172
[5] Aloraie A, Al-Mazrouee A, Price J W H, et al. Weld repair practices without post weld heat treatment for ferritic alloys and their consequences on residual stresses: a review[J]. International Journal of Pressure Vessels and Piping, 2010, 87: 127 - 133.
[6] 黄岚, 金硪馨. 1 000 MW汽轮机精加工转子轴颈微弧等离子堆焊研究[J]. 东方汽轮机, 2011(1): 21 - 25
Huang Lan, Jin Woxing. Study on micro-arc plasma deposition for finished rotor journal of 1 000 MW steam turbine[J]. Dongfang Turbine, 2011(1): 21 - 25
[7] 徐俊强, 彭勇, 刘智慧, 等. 等离子弧异质异构增材制造构件的组织与力学性能分析[J]. 焊接学报, 2019, 40(11): 119 - 124
Xu Junqiang, Peng Yong, Liu Zhihui, et al. Study on plasma arc additive manufacturing process of dissimilar steels with various composite structures[J]. Transactions of the China Welding Institution, 2019, 40(11): 119 - 124
[8] 中国机械工程学会焊接分会. 焊接手册[M]. 北京: 机械工业出版社, 2007.
Welding Society of China Mechanical Engineering Society.Welding Manual[M]. Beijing: China Mechanical Industry Press, 2007.
[9] 钟玉, 曹天兰, 梁刚, 等. 30Cr2Ni4MoV, 20Cr2NiMo和Cr2Ni2MoV材料的焊接性研究[J]. 东方汽轮机, 2012(2): 27 - 32
Zhong Yu, Cao Tianlan, Liang Gang, et al. Study on the weldability of 30Cr2Ni4MoV, 20Cr2NiMo and Cr2Ni2MoV materials[J]. Dongfang Turbine, 2012(2): 27 - 32
[10] Yan C Y, Jiang X Y, yuan Y, et al. Cold cracking susceptibility of X100 pipeline steel[J]. China Welding, 2019, 28(3): 1 - 9.
[11] 郭伟, 牛靖, 张建勋. 试样厚度对微冲剪试验结果的影响[J]. 焊接, 2012(5): 31 - 34
Guo Wei, Niu Jing, Zhang Jianxun. The influence of specimen thickness on the results of micro punching shear test[J]. Welding & Joining, 2012(5): 31 - 34
[12] Mohammad J E, Reza Alizadeh, Reza M. Applicability of shear punch testing to the evaluation of hot tensile deformation parameters and constitutive analyses[J]. Journal of Materials Research and Technology, 2019, 8(1): 996 - 1002.
[13] Tomasz K, Konrad G, Wojciech S, et al. Correlation between process parameters, microstructure and properties of 316 L stainless steel processed by selective laser melting[J]. Materials Science & Engineering A, 2018, 71: 64 - 73.
[14] Morteza S, Abbas E, Masoomeh E, et al. Interface microstructure across cladding of super duplex stainless steel with austenitic stainless steel buffer layer[J]. Surface & Coatings Technology, 2014, 259: 532 - 542.
[15] Wu Q J, Lu F G, Cui H C, et al. Soft zone formation by carbon migration and its effect onthe high-cycle fatigue in 9%Cr–CrMoV dissimilar welded joint[J]. Materials Letters, 2015, 141: 242 - 244.
[16] 王天剑, 黄菊, 张邦强, 等. 铬钼钢与巴氏合金摩擦磨损试验[J]. 大型铸锻件, 2009, 6: 11 - 14
Wang Tianjian, Huang Ju, Zhang Bangqiang, et al. Friction and wear test of Cr Mo steel and Babbitt alloy[J]. Heavy Castings and Forgings, 2009, 6: 11 - 14
[17] Guduru R K, Darling K A, Kishore R, et al. Evaluation of mechanical properties using shear–punch testing[J]. Materials Science and Engineering A, 2005, 395: 307 - 314.
[18] Foletti S, Madia M, Cammi A, et al. Characterization of the behavior of a turbine rotor steel by inverse analysis on the small punch test[J]. Procedia Engineering, 2011(10): 3628 - 3635.
[19] 潘超锋, 潘慧斌. 汽轮机转子输出端强度计算与校核[J]. 热力透平, 2017, 46(4): 46 - 49
Pan Chaofeng, Pan Huibin. Strength calculation and check of turbine rotor output end[J]. Thermal Turbine, 2017, 46(4): 46 - 49
[20] Li S, Ren S, Zhang Y, et al. Numerical investigation of formation mechanism of welding residual stress in P92 steel multi-pass joints[J]. Journal of Materials Processing Technology, 2017, 244: 240 - 252.
Outlines

/