综述

钨基合金与钢异质材料连接研究进展

  • 徐宇欣 ,
  • 邱小明 ,
  • 阮野 ,
  • 王苏煜 ,
  • 赵小辉 ,
  • 邢飞
展开
  • 吉林大学, 长春, 130025
徐宇欣,博士;主要研究方向为钨合金与异质材料连接; Email: xyx19@mails.jlu.edu.cn

收稿日期: 2020-12-08

  网络出版日期: 2022-02-22

基金资助

吉林省科技发展计划(20170204026GX);吉林大学中央高校基本科研业务费项目(451200318004)

Review on the research of the joining of tungsten based alloy and steel dissimilar materials

  • XU Yuxin ,
  • QIU Xiaoming ,
  • RUAN Ye ,
  • WANG Suyu ,
  • ZHAO Xiaohui ,
  • XING Fei
Expand
  • Jilin University, Changchun, 130025, China

Received date: 2020-12-08

  Online published: 2022-02-22

摘要

钨基合金具有高熔点、高强度、低热膨胀系数等优异性能,钢是目前应用最广泛的结构材料,钨基合金与钢连接形成结构部件在核工业的聚变反应堆与压铸模具等领域具有广阔的应用前景. 钨与钢的物理、化学、力学性能差异巨大,发展钨基合金与钢高性能连接存在一定挑战,且已成为焊接领域关键问题. 文中综合阐述了钨基合金与钢扩散焊、钎焊的研究现状,并结合应用需求,提出了钨基合金与钢异质金属连接的未来展望,为后续研究提供了相关参考.

本文引用格式

徐宇欣 , 邱小明 , 阮野 , 王苏煜 , 赵小辉 , 邢飞 . 钨基合金与钢异质材料连接研究进展[J]. 焊接学报, 2021 , 42(10) : 87 -96 . DOI: 10.12073/j.hjxb.20201208003

Abstract

Tungsten-based alloy has excellent properties such as high melting point, high strength, and low thermal expansion coefficient. Steel is still the most widely used metal material at present. The structural parts formed by tungsten-based alloy and steel have broad application prospects in fusion reactors, die-casting molds and other fields. Due to the huge differences in the physical, chemical and mechanical properties of tungsten and steel, the high-performance joining of tungsten-based alloy and steel is a great challenge and a key issue in the field of joining. In this paper, we reviewed the development of the brazing and diffusion bonding of tungsten-based alloys and steels. Additionally, in order to provide reference for subsequent research, the possible future research directions of tungsten-based alloy/steel dissimilar materials joining were proposed combined with the application requirements.

参考文献

[1] Singh P S, Liang Z, Pharr G M, et al. Creep of a thermally stable nanocrystalline nickel tungsten alloy as measured by high temperature nanoindentation[J]. Materials Science and Engineering:A, 2020, 784: 139309.
[2] Ravi Kiran U, Prabhu G, Nandy T K. Cooling rate effects on microstructure and mechanical behaviour of tungsten heavy alloys[J]. Materials Today:Proceedings, 2020, 26: 1631 ? 1637.
[3] Laas T, Laas K, Paju J, et al. Behaviour of tungsten alloy with iron and nickel under repeated high temperature plasma pulses[J]. Fusion Engineering and Design, 2020, 151: 111408.
[4] Jiao Z, Kang R, Dong Z, et al. Microstructure characterization of W-Ni-Fe heavy alloys with optimized metallographic preparation method[J]. International Journal of Refractory Metals and Hard Materials, 2019, 80: 114 ? 122.
[5] Pasalic M, Rustempasic F, Iyengar S, et al. Fatigue testing and microstructural characterization of tungsten heavy alloy Densimet 185[J]. International Journal of Refractory Metals and Hard Materials, 2014, 42: 163 ? 168.
[6] Ding L, Xiang D P, Pan Y L, et al. Mechanical properties and microstructural evolution of Mo-Co-co-strengthened W-Ni-Fe alloys by spark plasma sintering[J]. Journal of Alloys and Compounds, 2017, 712: 593 ? 598.
[7] Tang D, Zou S, Yan L. Influence of microelement Hf on microstructure, mechanical properties and shielding effect of W-Ni-Fe alloy[J]. Journal of Alloys and Compounds, 2017, 724: 1176 ? 1183.
[8] Prado J, Sánchez M, Wirtz M, et al. High heat flux performance of W-Eurofer brazed joints[J]. Journal of Nuclear Materials, 2018, 499: 225 ? 232.
[9] Das J, Appa Rao G, Pabi S K. Microstructure and mechanical properties of tungsten heavy alloys[J]. Materials Science and Engineering:A, 2010, 527(29-30): 7841 ? 7847.
[10] Batra I S, Kale G B, Saha T K, et al. Diffusion bonding of a Cu–Cr–Zr alloy to stainless steel and tungsten using nickel as an interlayer[J]. Materials Science and Engineering:A, 2004, 369(1-2): 119 ? 123.
[11] Vercruysse F, Celada-Casero C, Linke B M, et al. The effect of Nb on the strain rate and temperature dependent behaviour of quenching & partitioning steels[J]. Materials Science and Engineering:A, 2021, 800: 140293.
[12] Cui B, Yan P P, Du Q B, et al. The welding application of high strength steels used in engineering machinery[J]. China Welding, 2021, 30(1): 57 ? 64.
[13] Chen W, Gao P, Wang S, et al. Strengthening mechanisms of Nb and V microalloying high strength hot-stamped steel[J]. Materials Science and Engineering:A, 2020, 797: 140115.
[14] Prado J, Sánchez M, Wirtz M, et al. Impact of thermal fatigue on W–W brazed joints for divertor components[J]. Journal of Materials Processing Technology, 2018, 252: 211 ? 216.
[15] Tejado E, Prado J, Tarancón S, et al. Thermomechanical characterisation of W-Eurofer 97 brazed joints[J]. Journal of Nuclear Materials, 2020, 542: 152504.
[16] Huang P, Wang Y, Peng H, et al. Diffusion bonding W and RAFM-steel with an Fe interlayer by hot isostatic pressing[J]. Fusion Engineering and Design, 2020, 158: 111796.
[17] Lu C, Wang Y, Lei X, et al. Influence of Fe-W intermetallic compound on fracture behavior of steel/tungsten HIP diffusion bonding joint: Experimental investigation and first-principles calculation[J]. Journal of Manufacturing Processes, 2020, 55: 131 ? 142.
[18] Yang J, Wang Y, Huang J, et al. First-principles calculations on Ni/W interfaces in steel/Ni/W hot isostatic pressure diffusion bonding layer[J]. Applied Surface Science, 2019, 475: 906 ? 916.
[19] Yan H, Fan J, Han Y, et al. Vacuum diffusion bonding W to W-Cu composite: Interfacial microstructure and mechanical properties[J]. Vacuum, 2019, 165: 19 ? 25.
[20] Wang J C, Huang J, Sun H, et al. Effect of deuterium on bonding quality of W/Ti/steel HIP joints in first wall application[J]. Fusion Engineering and Design, 2019, 138: 313 ? 320.
[21] Tokitani M, Hamaji Y, Hiraoka Y, et al. Deformation and fracture behavior of the W/ODS-Cu joint fabricated by the advanced brazing technique[J]. Fusion Engineering and Design, 2019, 146: 1733 ? 1736.
[22] Yang L, Jiang X, Sun H, et al. Interfacial reaction and microstructure investigation of TC4/V/Cu/Co/316L diffusion-bonded joints[J]. Materials Letters, 2020, 261: 127140.
[23] Wang G, Sun X, Xu J, et al. Pressureless thermal diffusion bonding of transparent AlON ceramics by using a powder interlayer of parent material[J]. Scripta Materialia, 2019, 171: 118 ? 121.
[24] Pan H, Liu B, Guo Y, et al. An investigation on diffusion bonding of Zircaloy-4 and 304L stainless steel with Ti and Ag multiple interlayers[J]. Materials Letters, 2019, 240: 185 ? 188.
[25] Cavaleiro A J, Ramos A S, Braz Fernandes F M, et al. Follow-up structural evolution of Ni/Ti reactive nano and microlayers during diffusion bonding of NiTi to Ti6Al4V in a synchrotron beamline[J]. Journal of Materials Processing Technology, 2020, 275: 116354.
[26] Bachurina D, Suchkov A, Kalin B, et al. Joining of tungsten with low-activation ferritic–martensitic steel and vanadium alloys for demo reactor[J]. Nuclear Materials and Energy, 2018, 15: 135 ? 142.
[27] Basuki W W, Aktaa J. Investigation of tungsten/Eurofer 97 diffusion bonding using Nb interlayer[J]. Fusion Engineering and Design, 2011, 86(9-11): 2585 ? 2588.
[28] Basuki W W, Aktaa J. Diffusion bonding between W and Eurofer 97 using V interlayer[J]. Journal of Nuclear Materials, 2012, 429(1-3): 335 ? 340.
[29] Ma Y, Zhu W, Cai Q, et al. Microstructural evolution and mechanical properties in the partial transient liquid phase diffusion bonding of tungsten to steel[J]. International Journal of Refractory Metals and Hard Materials, 2018, 73: 91 ? 98.
[30] Cai Q, Liu W, Ma Y, et al. Effect of joining temperature on the microstructure and strength of W–steel HIP joints with Ti/Cu composite interlayer[J]. Journal of Nuclear Materials, 2018, 507: 198 ? 207.
[31] Cai Q, Liu W, Zhao Z, et al. Investigation of tungsten/steel diffusion bonding with Ni–Fe cladding on tungsten substrate[J]. Fusion Engineering and Design, 2017, 125: 189 ? 194.
[32] Cai Q, Liu W, Ma Y, et al. Microstructure, residual stresses and mechanical properties of diffusion bonded tungsten–steel joint using a V/Cu composite barrier interlayer[J]. International Journal of Refractory Metals and Hard Materials, 2015, 48: 312 ? 317.
[33] Basuki W W, Aktaa J. Process optimization for diffusion bonding of tungsten with Eurofer 97 using a vanadium interlayer[J]. Journal of Nuclear Materials, 2015, 459: 217 ? 224.
[34] 陈帅, 王玥, 杨健, 等. V/Nb 复合中间层热等静压扩散连接钢/钨接头的组织与性能[J]. 焊接学报, 2020, 41(11): 47 ? 53
Chen Shuai, Wang Yue, Yang Jian, et al. Microstructure and properties of hot isostatic pressing diffusion bonding steel/tungsten joint with V/Nb composite interlayer[J]. Thansactions of the China Welding Institution, 2020, 41(11): 47 ? 53
[35] Liu W, Pang X, Cai Q, et al. Fabrication of W/steel joint using hot isostatic pressing with Ti/Cu/Ti liquid forming interlayer[J]. Fusion Engineering and Design, 2018, 135: 59 ? 64.
[36] Liu W, Wang Z, Ma Y, et al. Investigation of tungsten/steel brazing using Ta and Cu interlayer[J]. Fusion Engineering and Design, 2016, 113: 102 ? 108.
[37] Liu W, Sheng Q, Ma Y, et al. Interfacial microstructures, residual stress and mechanical analysis of hot isostatic pressing diffusion bonded joint of 93W–4.9Ni–2.1Fe alloy and 30CrMnSiNi2A steel[J]. Fusion Engineering and Design, 2020, 156: 111602.
[38] Wang Y, Chen S, Lei X, et al. Interfacial structure and formation mechanism of tungsten/steel HIP diffusion bonding joints using Ni interlayer[J]. Journal of Manufacturing Processes, 2020, 52: 235 ? 246.
[39] Rieth M, Dudarev S L, Gonzalez de Vicente S M, et al. Recent progress in research on tungsten materials for nuclear fusion applications in Europe[J]. Journal of Nuclear Materials, 2013, 432(1-3): 482 ? 500.
[40] Wang Y, Yang J, Huang J, et al. Hot isostatic diffusion bonding tungsten alloy and high-strength steel Part I: Design and preparation of Ni-Si-B interlayer by magnetron sputtering[J]. Journal of Manufacturing Processes, 2018, 35: 360 ? 367.
[41] Zhu W, Qiang J, Wang Y, et al. A Ti-Fe-Sn thin film assembly for joining tungsten and reduced activation ferritic-martensitic steels[J]. Materials & Design, 2017, 125: 55 ? 61.
[42] Dourandish M, Simchi A, Hokamoto K, et al. Interface formation and bond strength in 3Y-TZP/Cr composite bilayers produced by sinter–joining[J]. Materials Science and Engineering:A, 2010, 527(3): 449 ? 453.
[43] Firouzdor V, Simchi A, Kokabi A H. An investigation of the densification and microstructural evolution of M2/316L stepwise graded composite during co-sintering[J]. Journal of Materials Science, 2007, 43(1): 55 ? 63.
[44] Liu W, Zhang L, Ma Y, et al. Low temperature co–sintering of tungsten alloy/steel composite structure[J]. International Journal of Refractory Metals and Hard Materials, 2020, 90: 105224.
[45] Prado J, Sánchez M, Stan G, et al. Effect of Cr and V coatings on W base material in W-Eurofer brazed joints for fusion applications[J]. Fusion Engineering and Design, 2020, 159: 111748.
[46] Chehtov T, Aktaa J, Kraft O. Mechanical characterization and modeling of brazed Eurofer-tungsten-joints[J]. Journal of Nuclear Materials, 2007, 367-370: 1228 ? 1232.
[47] Oono N, Noh S, Iwata N, et al. Microstructures of brazed and solid-state diffusion bonded joints of tungsten with oxide dispersion strengthened steel[J]. Journal of Nuclear Materials, 2011, 417(1-3): 253 ? 256.
[48] Sánchez M, Garrido M A, Múnez C J, et al. Analysis of the brazeability of W–W joints using a high temperature Ni-based alloy[J]. Materials & Design, 2014, 54: 900 ? 905.
[49] Shang J, Yan J, Li N. Brazing W and Fe–Ni–Co alloy using Ag–28Cu and Ag–27Cu–3.5Ti fillers[J]. Journal of Alloys and Compounds, 2014, 611: 91 ? 95.
[50] Prado J, Sánchez M, Ruiz A, et al. Effect of brazing temperature, filler thickness and post brazing heat treatment on the microstructure and mechanical properties of W-Eurofer joints brazed with Cu interlayers[J]. Journal of Nuclear Materials, 2020, 533: 152117.
[51] Prado J, Sánchez M, Antusch S, et al. Development of a brazing procedure to join W-2Y2O3 and W-1TiC PIM materials to Eurofer[J]. Physica Scripta, 2020, T171: 014022.
[52] Prado J, Sánchez M, Ure?a A. Wettability study of a Cu-Ti alloy on tungsten and Eurofer substrates for brazing components of DEMO fusion reactor[J]. Materials & Design, 2016, 99: 93 ? 101.
[53] Prado J, Sánchez M, Ure?a A. Evaluation of mechanically alloyed Cu-based powders as filler alloy for brazing tungsten to a reduced activation ferritic-martensitic steel[J]. Journal of Nuclear Materials, 2017, 490: 188 ? 196.
[54] Prado J, Roldán M, Sánchez M, et al. Interfacial characterization by TEM and nanoindentation of W-Eurofer brazed joints for the first wall component of the DEMO fusion reactor[J]. Materials Characterization, 2018, 142: 162 ? 169.
[55] Zhu D, Xu H, Dong D, et al. Brazing of (TiB + Y2O3) reinforced titanium matrix composites using CuTiZrNi amorphous filler alloy[J]. Vacuum, 2020, 174: 109212.
[56] Xia Y, Dong H, Zhang R, et al. Interfacial microstructure and shear strength of Ti6Al4V alloy/316 L stainless steel joint brazed with Ti33.3Zr16.7Cu50?xNix amorphous filler metals[J]. Materials & Design, 2020, 187: 108380.
[57] Xia Y, Dong H, Li P. Brazing TC4 titanium alloy/316L stainless steel joint with Ti50-xZrxCu39Ni11 amorphous filler metals[J]. Journal of Alloys and Compounds, 2020, 849: 156650.
[58] Li C, Zhang K, Mao X, et al. Microstructure and mechanical properties of the AlON / Ti6Al4V active element brazing joint[J]. Materials Science and Engineering:A, 2020, 793: 139859.
[59] Xia Y, Dong H, Hao X, et al. Vacuum brazing of Ti6Al4V alloy to 316L stainless steel using a Ti-Cu-based amorphous filler metal[J]. Journal of Materials Processing Technology, 2019, 269: 35 ? 44.
[60] Zhang T, Yang X, Miao K, et al. Microstructure evolution and brazing mechanism of Ti5Si3/Ti3Al composite and Ni-based superalloy joints using Ti-Zr-Cu-Ni filler alloy[J]. Materials Science and Engineering:A, 2018, 713: 28 ? 34.
[61] Dong H, Yang Z, Wang Z, et al. CuTiNiZrV amorphous alloy Foils for vacuum brazing of TiAl alloy to 40Cr steel[J]. Journal of Materials Science & Technology, 2015, 31(2): 217 ? 222.
[62] Wang J B, Lian Y Y, Feng F. Microstructure of the tungsten and reduced activation ferritic-martensitic steel joint brazed with an Fe-based amorphous alloy[J]. Fusion Engineering and Design, 2019, 138: 164 ? 169.
[63] Bachurina D, Suchkov A, Filimonov A, et al. High-temperature brazing of tungsten with steel by Cu-based ribbon brazing alloys for DEMO[J]. Fusion Engineering and Design, 2019, 146: 1343 ? 1346.
[64] 杨宗辉, 沈以赴, 初雅杰, 等. 钴/镍复合中间层真空扩散连接钨与钢[J]. 焊接学报, 2020, 41(3): 54 ? 58
Yang Zonghui, Shen Yifu, Chu Yajie, et al. Tungsten/steel vacuum diffusion bonding using Co/Ni composite interlayer[J]. Thansactions of the China Welding Institution, 2020, 41(3): 54 ? 58
[65] 杨宗辉, 沈以赴, 初雅杰, 等. Cu/W-Ni-Co/Ni多中间层的钨/钢扩散连接[J]. 稀有金属材料与工程, 2015, 44(344): 192 ? 196
Yang Zonghui, Shen Yifu, Chu Yajie, et al. Diffusion bonding between tungsten and steel with Cu/W-Ni-Co/Ni multi-interlayer[J]. rare metal materials and engineering, 2015, 44(344): 192 ? 196
[66] 徐振钦, 杨宗辉. 异种材料焊接接头热应力缓冲中间层的研究现状[J]. 机械工程材料, 2013, 37(301): 10 ? 14,19
Xu Zhenqin, Yang Zonghui. Research actuality of thermal stress relaxation interlayer for dissimilar materials joints[J]. Materials for Mechanical Engineering, 2013, 37(301): 10 ? 14,19
[67] Wang Y, Wang W, Ye Z, et al. Reactive composite-diffusing brazing of Cf/SiC composite and stainless steel with (Cu–15Ti)+C filler material[J]. Materials Science and Engineering:A, 2020, 788: 139582.
[68] Wang W, Fan D, Huang J, et al. Microstructural mechanism and mechanical properties of Cf/SiC composite/TC4 alloy joints composite-diffusion brazed with TiZrCuNi?+?TiCp composite filler[J]. Materials Science and Engineering:A, 2018, 728: 1 ? 9.
[69] Cui B, Huang J, Cai C, et al. Microstructures and mechanical properties of Cf/SiC composite and TC4 alloy joints brazed with (Ti–Zr–Cu–Ni)+W composite filler materials[J]. Composites Science and Technology, 2014, 97: 19 ? 26.
[70] Xu Y X, Qiu X M, Wang S Y, et al. Interfacial microstructure and mechanical properties of tungsten based powder alloy and superalloy GH907 diffusion brazing joint with Cu-Ni-V-Ti interlayer[J]. Vacuum, 2021, 184: 109793.
[71] Cai Q S, Zhu W T, Ma Y Z, et al. Rational design of composite interlayer for diffusion bonding of tungsten–steel joints[J]. International Journal of Refractory Metals and Hard Materials, 2018, 70: 155 ? 161.
文章导航

/